Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
melt mass-flow rate | | ISO 1133 | 4.0 g/10min |
Environmental stress cracking resistance | | ASTM D1693 | 400 hr |
Environmental stress cracking resistance | | ASTM D1693 | >1000 hr |
hardness | Test Condition | Test Method | Test Result |
---|
Shore hardness | | ISO 868 | 57 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | ISO 527-2 | 17.0 Mpa |
tensile strength | | ISO 527-2 | 17.0 Mpa |
tensile strength | | ISO 527-2 | 21.8 Mpa |
tensile strength | | ISO 527-2 | 24.7 Mpa |
Tensile strain | | ISO 527-2 | 700 % |
Tensile strain | | ISO 527-2 | 800 % |
Flexural modulus | | ISO 178 | 640 Mpa |
tear strength | | DIN 53515 | 140 Mpa |
tear strength | | DIN 53515 | 145 Mpa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Multi axis Instrumented Impact Energy | | ISO 6603-2 | 23.0 J |
Multi axis Instrumented Impact Energy | | ISO 6603-2 | 17.0 J |
Multi axis Instrumented Impact Energy | | ISO 6603-2 | 17.0 J |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Crystallization peak temperature | | DSC | 105 °C |
Heat distortion temperature | | ISO 75-2/A | 38.9 °C |
vicat | | ISO 306/A120 | 118 °C |
melting temperature | | DSC | 125 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.