Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | | 1.20 g/cm³ |
Melt volume flow rate | | ISO1133 | 50.0 cm³/10min |
Melt volume flow rate | | ISO1133 | 6.00 cm³/10min |
Melt volume flow rate | | ISO1133 | 0.40到0.70 % |
water content | | 内部方法 | <0.20 % |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | V-0 |
Burning wire flammability index | | IEC60695-2-12 | 750 °C |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of simply supported beam without notch | | ISO179/1eU | 42 kJ/m² |
Impact strength of simply supported beam without notch | | ISO179/1eU | 65 kJ/m² |
Impact strength of cantilever beam gap | | ISO180/1A | 4.0 kJ/m² |
Impact strength of cantilever beam gap | | ISO180/1A | 10 kJ/m² |
| | ISO180 | 40 kJ/m² |
| | ISO180 | 40 kJ/m² |
Charpy Notched Impact Strength | | ISO179/1eA | 4.0 kJ/m² |
Charpy Notched Impact Strength | | ISO179/1eA | 9.0 kJ/m² |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ISO527-2 | 2300 MPa |
Tensile stress | | ISO527-2 | 40.0 MPa |
Tensile strain | | ISO527-2 | 15 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|
BallPressure Test | | IEC60335-1 | 通过 |
| | ISO75-2/A | 82.0 °C |
vicat | | ISO306/B50 | 93.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.