PS SECCO HIPS-622S Shanghai SECCO Petrochemical Co., Ltd
0
- Usages:Bottles food packaging cups
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 11 kJ/m² |
| flammability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| UL flame retardant rating | UL 94 | HB |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | Yield | ISO 527-2/50 | 26.0 MPa |
| bending strength | ISO 178 | 40.0 MPa | |
| Bending modulus | ISO 178 | 1650 MPa | |
| Nominal tensile fracture strain | ISO 527-2/50 | 60 % | |
| tensile strength | Break | ISO 527-2/50 | 25.0 MPa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Vicat softening temperature | ISO 306/B50 | 90.0 °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 72.0 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Water absorption rate | Saturation,23°C | ISO 62 | <0.10 % |
| Shrinkage rate | 24hr | ISO 294-4 | 0.40to0.60 % |
| melt mass-flow rate | 200°C/5.0kg | ISO 1133 | 3.6 g/10min |
| density | ISO 1183 | 1.04 g/cm³ |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Rockwell hardness | R-Sale | ISO 2039-2 | 97 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.