plas
Log In

PC/PET Eastalloy™ DA003-8906K EASTMAN USA

17

Technical Data Sheet

optical performanceTest ConditionTest MethodTest Result
turbidityASTM D10033.6 %
transmissivityRegularASTM D100377.0 %
transmissivityTotalASTM D100381.0 %
impact performanceTest ConditionTest MethodTest Result
Dart impact-40°C,EnergyatPeakLoadASTM D376346.0 J
Dart impact23°C,EnergyatPeakLoadASTM D376351.0 J
Multi axis Instrumented Impact Energy-40°C,能量to力量峰值ISO 6603-223.0 J
Multi axis Instrumented Impact Energy23°C,能量to力量峰值ISO 6603-219.0 J
flammabilityTest ConditionTest MethodTest Result
UL flame retardant rating3.2mmUL 94V-2
UL flame retardant rating1.6mmUL 94HB
mechanical propertiesTest ConditionTest MethodTest Result
Bending modulus4.00mmISO 1782100 Mpa
Bending modulusASTM D7902140 Mpa
Tensile strainBreak,4.00mmISO 527-2130 %
elongationBreakASTM D638150 %
Tensile strainYield,4.00mmISO 527-25.4 %
elongationYieldASTM D6386.0 %
tensile strengthBreak,4.00mmISO 527-256.0 Mpa
tensile strengthBreakASTM D63860.0 Mpa
tensile strengthYield,4.00mmISO 527-256.0 Mpa
tensile strengthYieldASTM D63856.0 Mpa
bending strength4.00mmISO 17881.0 Mpa
bending strengthYieldASTM D79086.0 Mpa
thermal performanceTest ConditionTest MethodTest Result
specific heat240°CDSC2180 J/kg/°C
specific heat60°CDSC1380 J/kg/°C
Vicat softening temperature--ISO 306/B110 °C
Hot deformation temperature0.45MPa,UnannealedASTM D648103 °C
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B103 °C
Hot deformation temperature1.8MPa,UnannealedASTM D64890.0 °C
Hot deformation temperature1.8MPa,UnannealedISO 75-2/A90.0 °C
Vicat softening temperatureASTM D15252118 °C
Vicat softening temperature--ISO 306/A118 °C
Physical propertiesTest ConditionTest MethodTest Result
Shrinkage rateMD:3.20mmASTM D9550.50-0.70 %
Water absorption rate24hrASTM D5700.13 %
Water absorption rate23°C,24hrISO 620.13 %
Electrical performanceTest ConditionTest MethodTest Result
Dissipation factor1kHzASTM D1502E-03
Dissipation factor1MHzASTM D1508E-03
Arc resistanceASTM D495143 sec
Dielectric constant1MHzASTM D1502.10
Dielectric constant1kHzASTM D1502.30
Dielectric strengthASTM D14917 KV/mm
Volume resistivityASTM D2571E+15 ohms·cm
Surface resistivityASTM D2571E+16 ohms
High voltage arc tracing rateHVTRUL 746PLC 2 mm/min
Compared to the anti leakage trace indexASTM D3638PLC 0
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessR-ScaleASTM D785117
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.