Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTM D792 | 1.25 g/cm³ |
density | | ISO 1183 | 1.25 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
DurometerHardness | | ASTM D2240 | 70 |
IRHD hardness | | ISO 48 | 70 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ASTM D638 | 3.93 MPa |
Tensile modulus | | ISO 527-2 | 3.93 MPa |
tensile strength | | ASTM D638 | 8.83 MPa |
tensile strength | | ISO 527-2 | 8.83 MPa |
Tensile strain | | ASTM D638 | 440 % |
Tensile strain | | ISO 527-2 | 440 % |
Taber abraser | | ASTM D1044 | 4.00 mg |
elastomer | Test Condition | Test Method | Test Result |
---|
Clash Mountain Module | | ASTM D1043 | 68.9 MPa |
Stretch permanent deformation | | ASTM D412 | 9 % |
tear strength | | ASTM D624 | 38.5 kN/m |
compression set | | ASTM D395B | 21 % |
compression set | | ASTM D395B | 74 % |
compression set | | ISO 815 | 21 % |
compression set | | ISO 815 | 74 % |
aging | Test Condition | Test Method | Test Result |
---|
volume change | | ASTM D471 | -17 % |
volume change | | ASTM D471 | 17 % |
volume change | | ASTM D471 | 11 % |
Shore hardness | | ISO 188 | 64 |
elongation at break | | ASTM D471 | 380 % |
Hardness change rate in the air | | ASTM D471 | 64 |
volume change | | ASTM D471 | 16 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|
brittle temperature | | ASTM D746 | -60.0 °C |
brittle temperature | | ISO 974 | -60.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.