plas
Log In

PA66 AR-17 (P) ADELL USA

6
  • Properties:
    enhanceGlass fiber reinforcedFiller: Glass fiber reinf33% filler by weight
  • Compare

Technical Data Sheet

mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthYieldASTM D638214 Mpa
elongationBreakASTM D6383.0 %
Bending modulusASTM D7909650 Mpa
bending strengthYieldASTM D790283 Mpa
compressive strengthASTM D695245 Mpa
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature0.45MPa,UnannealedASTM D648249 °C
Hot deformation temperature1.8MPa,UnannealedASTM D648249 °C
Hot deformation temperatureMelting TemperatureASTM D648254to271 °C
Linear coefficient of thermal expansionMDASTM D6962.3E-05 cm/cm/°C
thermal conductivityASTMC1770.50 W/m/K
Physical propertiesTest ConditionTest MethodTest Result
Shrinkage rateMDASTM D9550.20-0.50 %
Water absorption rate24hrASTM D5700.70 %
Electrical performanceTest ConditionTest MethodTest Result
Volume resistivityASTM D2571E+15 ohms·cm
Dielectric strengthASTM D14921 KV/mm
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessM-ScaleASTM D785101
Rockwell hardnessR-ScaleASTM D785123
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.