PA66 AR-17 (P) ADELL USA
--
--
enhance、Glass fiber reinforced、Filler: Glass fiber reinf、33% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | ADELL USA/AR-17 (P) |
---|---|---|---|
Rockwell hardness | M级 | ASTM D785 | 101 |
R级 | ASTM D785 | 123 |
Electrical performance | Test Condition | Test Method | ADELL USA/AR-17 (P) |
---|---|---|---|
Volume resistivity | ASTM D257 | 1E+15 ohms·cm | |
dielectric strength | ASTM D149 | 21 KV/mm |
Mechanical properties | Test Condition | Test Method | ADELL USA/AR-17 (P) |
---|---|---|---|
elongation | 断裂 | ASTM D638 | 3.0 % |
bending strength | 屈服 | ASTM D790 | 283 Mpa |
tensile strength | 屈服 | ASTM D638 | 214 Mpa |
Flexural modulus | ASTM D790 | 9650 Mpa | |
compressive strength | ASTM D695 | 245 Mpa |
physical property | Test Condition | Test Method | ADELL USA/AR-17 (P) |
---|---|---|---|
Shrinkage rate | MD | ASTM D955 | 0.20-0.50 % |
Water absorption rate | 24hr | ASTM D570 | 0.70 % |
Thermal performance | Test Condition | Test Method | ADELL USA/AR-17 (P) |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 249 °C |
0.45MPa,未退火,HDT | ASTM D648 | 249 °C | |
熔融温度,HDT | ASTM D648 | 254to271 °C | |
thermal conductivity | ASTMC177 | 0.50 W/m/K | |
Linear coefficient of thermal expansion | MD | ASTM D696 | 2.3E-05 cm/cm/°C |