Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| thermal performance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3GF33 |
|---|---|---|---|
| Melting temperature | DIN EN11357-1 | 262 °C | |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 260 °C |
| 8.0MPa,Unannealed | ISO 75-2/C | 220 °C | |
| 1.8MPa,Unannealed | ISO 75-2/A | 255 °C | |
| Electrical performance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3GF33 |
| Volume resistivity | IEC 60093 | 1E+13 ohms·cm | |
| Compared to the anti leakage trace index | SolutionA | IEC 60112 | PLC 0 |
| Surface resistivity | IEC 60093 | 1E+12 ohms | |
| mechanical properties | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3GF33 |
| Tensile strain | Break | ISO 527-2/5 | 3.0 % |
| Tensile modulus | ISO 527-2/1 | 11500 Mpa | |
| tensile strength | Break | ISO 527-2/5 | 210 Mpa |
| Physical properties | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3GF33 |
| Water absorption rate | Saturation,23°C | ISO 62 | 4.7to5.3 % |
| Hygroscopicity | 70°C,62%RH | ISO 1110 | 1.8to2.0 % |
| flammability | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3GF33 |
| UL flame retardant rating | 1.6mm | UL 94 | HB |
| Burning rate | 1.00mm | FMVSS302 | <100 mm/min |
| Supplementary Information | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3GF33 |
| ReinforcementContent | ISO 1172 | 33 % | |
| impact performance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3GF33 |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 80 kJ/m² |
| -30°C | ISO 179/1eU | 80 kJ/m² |