Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Reference Price
| impact performance | Test Condition | Test Method | PRIME POLYMER JAPAN/JR-3070HP |
|---|---|---|---|
| Impact strength of simply supported beam without notch | -20°C | ISO 179 | 2.5 kJ/m² |
| 23°C | ISO 179 | 7.5 kJ/m² | |
| thermal performance | Test Condition | Test Method | PRIME POLYMER JAPAN/JR-3070HP |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 65.0 °C |
| 0.45MPa | ISO 75 | 65 °C | |
| Basic Performance | Test Condition | Test Method | PRIME POLYMER JAPAN/JR-3070HP |
| melt mass-flow rate | 230℃ | ISO 1133 | 33 g/10min |
| density | ISO 1183 | 0.910 g/cm³ | |
| mechanical properties | Test Condition | Test Method | PRIME POLYMER JAPAN/JR-3070HP |
| tensile strength | Yield | ISO 527-2 | 20.0 Mpa |
| Tensile strain | Break | ISO 527-2 | 400 % |
| elongation | Break | ISO 527 | 400 % |
| Rockwell hardness | ISO 2039-2 | 49 R scale | |
| Tensile modulus | ISO 527-2 | 700 Mpa | |
| tensile strength | ISO 527 | 20.0 Mpa | |
| Bending modulus | ISO 527 | 700 Mpa | |
| Impact strength of cantilever beam gap | -20℃ | ISO 179 | 2.5 kJ/m² |
| 23℃ | ISO 179 | 7.5 kJ/m² | |
| hardness | Test Condition | Test Method | PRIME POLYMER JAPAN/JR-3070HP |
| Rockwell hardness | R-Sale | ISO 2039-2 | 49 |
| Physical properties | Test Condition | Test Method | PRIME POLYMER JAPAN/JR-3070HP |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 33 g/10min |