Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| mechanical properties | Test Condition | Test Method | CELANESE GERMANY/EC140 |
|---|---|---|---|
| Tensile modulus | ISO 527-2/1A/1 | 8500 Mpa | |
| tensile strength | Break | ISO 527-2/1A/5 | 70.0 Mpa |
| Bending modulus | 23°C | ISO 178 | 8500 Mpa |
| Tensile strain | Break | ISO 527-2/1A/5 | 1.5 % |
| other | Test Condition | Test Method | CELANESE GERMANY/EC140 |
| purpose | 用于工业用途 | ||
| characteristic | 耐磨 | ||
| Physical properties | Test Condition | Test Method | CELANESE GERMANY/EC140 |
| Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 12.0 cm3/10min |
| Shrinkage rate | MD | ISO 294-4 | 0.80 % |
| TD | ISO 294-4 | 1.0 % | |
| Electrical performance | Test Condition | Test Method | CELANESE GERMANY/EC140 |
| Volume resistivity | IEC 60093 | 2E+03 ohms·cm | |
| Surface resistivity | IEC 60093 | 1E+03 ohms | |
| thermal performance | Test Condition | Test Method | CELANESE GERMANY/EC140 |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 162 °C |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 1E-04 cm/cm/°C |
| MD | ISO 11359-2 | 3E-05 cm/cm/°C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 158 °C |
| Melting temperature | ISO 11357-3 | 165 °C |