| thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/420SEO-1001 |
|---|---|---|---|
| Linear coefficient of thermal expansion | 420SEO-1001 | 2.5E-05 1/℃ | |
| UL flame retardant rating | 5V mm | ||
| Long term use temperature | 无冲击 | 140 °C | |
| Hot deformation temperature | HDT | 215 °C | |
| Long term use temperature | 电气 | 130 °C | |
| 含冲击 | 130 °C | ||
| Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/420SEO-1001 |
| Water absorption rate | 0.06 % | ||
| density | 1.6 | ||
| enhance | 30 % | ||
| Shrinkage rate | 3-5 E-3 | ||
| mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/420SEO-1001 |
| Bending modulus | 7579 Mpa | ||
| Rockwell hardness | 119 | ||
| Impact strength of cantilever beam gap | 23℃ | 64 J/m | |
| tensile strength | Break | 117 Mpa | |
| Electrical performance | Test Condition | Test Method | SABIC INNOVATIVE US/420SEO-1001 |
| Dissipation factor | 0.02 | ||
| Volume resistivity | 4E+16 ohm-cm | ||
| Dielectric constant | 3.7 |