PBT 420SEO-1001 SABIC INNOVATIVE US
220
Form:Granules | Grade:Injection grade
Properties:
Glass fiber reinforceddimensional stability High rigidityhigh strengthheat-resistingCharacteristic: 30% GRUL94V-0/5V
Typical Applications:
Lawn equipmentGarden equipmentIndustrial applicationsAutomotive External PartsElectrical fieldElectronic fieldArchitectural application fieldOutdoor applicationsElectrical appliancesEngine hood partsMedical suppliesNursing suppliesPlastic bagAutomotive interior partsCastersHousehold goodsPetroleum ApplicationsNatural gas suppliessporting goodsTextile applicationLighting applicationsTrimming machinefood mixerMotor statorSwitches etc
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Lawn equipment | Garden equipment | Industrial applications | Automotive External Parts | Electrical field | Electronic field | Architectural application field | Outdoor applications | Electrical appliances | Engine hood parts | Medical supplies | Nursing supplies | Plastic bag | Automotive interior parts | Casters | Household goods | Petroleum Applications | Natural gas supplies | sporting goods | Textile application | Lighting applications | Trimming machine | food mixer | Motor stator | Switches | etc |
| Properties: | Glass fiber reinforced | dimensional stability | High rigidity | high strength | heat-resisting | Characteristic: 30% GR | UL94 | V-0/5V |
Certificates
No Data...
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23℃ | 64 | J/m | |
| Bending modulus | 7579 | Mpa | ||
| Rockwell hardness | 119 | |||
| tensile strength | Break | 117 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Long term use temperature | 含冲击 | 130 | °C | |
| 无冲击 | 140 | °C | ||
| UL flame retardant rating | 5V | |||
| 2.3 | mm | |||
| V-0 | ||||
| Hot deformation temperature | HDT | 215 | °C | |
| HDT | 204 | °C | ||
| Linear coefficient of thermal expansion | 420SEO-1001 | 2.5E-05 | 1/℃ | |
| UL flame retardant rating | 0.7 | mm | ||
| Long term use temperature | 电气 | 130 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | 3-5 | E-3 | ||
| enhance | 30 | % | ||
| density | 1.6 | |||
| Water absorption rate | 0.06 | % | ||
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric constant | 3.7 | |||
| Dissipation factor | 0.02 | |||
| Volume resistivity | 4E+16 | ohm-cm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.