| mechanical properties | Test Condition | Test Method | INVISTA SHANGHAI/U4820L NC01 |
|---|---|---|---|
| bending strength | ISO 178 | 96.0 Mpa | |
| tensile strength | Yield | ISO 527-2/50 | 82.0 Mpa |
| Tensile strain | Break | ISO 527-2 | 35 % |
| Bending modulus | ISO 178 | 3000 Mpa | |
| Tensile modulus | ISO 527-2/1 | 3200 Mpa | |
| Tensile strain | Yield | ISO 527-2 | 4.1 % |
| flammability | Test Condition | Test Method | INVISTA SHANGHAI/U4820L NC01 |
| Burning wire flammability index | 1.5mm | IEC 60695-2-12 | 960 °C |
| 3.0mm | IEC 60695-2-12 | 960 °C | |
| UL flame retardant rating | 0.40mm | UL 94 | V-2 |
| Hot filament ignition temperature | 0.71mm | IEC 60695-2-13 | 960 °C |
| Burning wire flammability index | 0.71mm | IEC 60695-2-12 | 960 °C |
| Hot filament ignition temperature | 1.5mm | IEC 60695-2-13 | 900 °C |
| 3.0mm | IEC 60695-2-13 | 750 °C | |
| impact performance | Test Condition | Test Method | INVISTA SHANGHAI/U4820L NC01 |
| Impact strength of simply supported beam without notch | -30°C | ISO 179 | NoBreak |
| 23°C | ISO 179 | NoBreak | |
| Electrical performance | Test Condition | Test Method | INVISTA SHANGHAI/U4820L NC01 |
| Volume resistivity | 2.00mm | IEC 60093 | 4E+14 ohms·cm |
| Surface resistivity | IEC 60093 | 3E+14 ohms | |
| Dielectric strength | 1.00mm | IEC 60243-1 | 32 KV/mm |
| Physical properties | Test Condition | Test Method | INVISTA SHANGHAI/U4820L NC01 |
| Water absorption rate | 23°C,24hr | ISO 62 | 1.7 % |
| Shrinkage rate | TD:2.00mm | ISO 294-4 | 1.8 % |
| MD:2.00mm | ISO 294-4 | 1.8 % | |
| thermal performance | Test Condition | Test Method | INVISTA SHANGHAI/U4820L NC01 |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 221 °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 71.0 °C | |
| Melting temperature | ISO 11357-3 | 262 °C |