thermal performanceTest ConditionTest MethodARKEMA CHANGSHU/720
decomposition temperatureTGA在空气中1 %质量损失内部测试方法375 °C
Melting temperatureASTM D3418165-172 °C
decomposition temperatureTGA在通气中1%质量损失内部测试方法410 °C
specific heat内部测试方法745-958 J/(kg.k)
Melting temperature10℃/minISO 11357168 °C
thermal conductivityASTM E14610.17-0.19 W/(m.K)
Hot deformation temperature1.8MPa120℃/hrASTM D648105-115 °C
Linear coefficient of thermal expansion23℃ASTM D6961.19E-3 cm/cm/℃
Glass transition temperatureASTM D7028-40.6-38.3 °C
Hot deformation temperature1.8MPaISO 75110 °C
Vicat softening temperature50℃/hr 50NISO 306139 °C
Glass transition temperature10℃/minISO 11357-40 °C
Hot deformation temperature0.45MPa120℃/hrASTM D648125-140 °C
Linear coefficient of thermal expansionFlowISO 113590.00015 m/m/k
Hot deformation temperature0.45MPaISO 75132 °C
Physical propertiesTest ConditionTest MethodARKEMA CHANGSHU/720
Water absorption rateASTM D5700.01-0.03 %
densityISO 11831780 kg/㎥
23℃ASTM D7921.77-1.79 g/㎤
Yirong Index230℃ 5kgISO 113310 ㎤/10min
Shrinkage rateFlowISO 2942 %
melt mass-flow rate230°C 3.8kgASTM D12385-26.5 g/10min
Shrinkage rate垂直ISO 2942 %
Water absorption rateISO 620.03 %
Melt viscosity230℃100sASTM D38356-12 kPoise
mechanical propertiesTest ConditionTest MethodARKEMA CHANGSHU/720
elongationYieldISO 5278 %
Impact strength of cantilever beam gap23℃ASTM D2560.0801-0.214 KJ/m
tensile strengthYieldISO 52754 Mpa
Compression slip23℃ASTM D69568.9-103 Mpa
elongationBreak23℃ASTM D63820-100 %
Bending modulus23℃ASTM D7901380-2310 Mpa
elongationYield23℃ASTM D638570 %
Suspended wall beam without notch impact strength23℃ASTM D2561.07-4.27 KJ/m
Tensile modulus23℃ASTM D6381380-2310 Mpa
tensile strengthBreak23℃ASTM D63834.5-55.2 Mpa
Charpy Notched Impact Strength23℃ISO 179208 kJ/㎡
tensile strengthYield23℃ASTM D63844.8-55.2 Mpa
Tensile modulusISO 5272200 Mpa
Charpy Notched Impact Strength-30℃ISO 179189 kJ/㎡
elongationBreakISO 52750 %
Charpy Notched Impact Strength-30°CISO 1795 kJ/㎡
Taber wear resistanceCS-17轮1kgASTM G1955-9 mg/1000cy
bending strength23℃5.0%StrainASTM D79058.6-75.8 Mpa
Friction coefficient静态 对钢23℃ASTM D18940.14
ULTest ConditionTest MethodARKEMA CHANGSHU/720
UL flame retardant rating1.5mmUL 94V-0
RTI Str本色 1.5mmUL 746B150 °C
Outdoor applicabilityUL -746Cf1
RTI Elec本色 1.5mmUL 746B150 °C
RTI Imp本色 1.5mmUL 746B150 °C
Electrical performanceTest ConditionTest MethodARKEMA CHANGSHU/720
Dielectric constant100HzIEC 602509
Dissipation factor100HzIEC 602500.032
Dielectric constantiKHzASTM D1504.5-9.5
Volume resistivity20℃ 65RHASTM D257200000000000000 Ω.cm
Dissipation factor1MHzIEC 602500.214
Surface resistivityIEC 600931000000000000000
Dielectric constant1MHzIEC 602507
Dielectric strengthIEC 6024321 KV/mm
Dissipation factor100kHzASTM D1500.01-0.21
Dielectric strength23℃ASTM D1491.7 KV/mm
Compared to the anti leakage trace indexIEC 60112PLC 0
Accumulation resistorIEC 600932000000000000 Ω.m
flame retardant performanceTest ConditionTest MethodARKEMA CHANGSHU/720
Extreme Oxygen IndexISO 458943 %
UL flame retardant rating1.5mmUL 94V-0
Extreme Oxygen IndexASTM D286344 %
optical performanceTest ConditionTest MethodARKEMA CHANGSHU/720
Refractive index钠光谱D线ASTM D5421.42
hardnessTest ConditionTest MethodARKEMA CHANGSHU/720
Shore hardness23℃ASTM D224076-80