| elastomer | Test Condition | Test Method | TOYOBO JAPAN/P40UX |
|---|---|---|---|
| Permanent compression deformation | JISK6301 | 50 % | |
| tear strength | ASTM D624 | 98.0 kN/m | |
| mechanical properties | Test Condition | Test Method | TOYOBO JAPAN/P40UX |
| elongation | Break | ASTM D638 | 690 % |
| Taber abraser | 1000Cycles | ASTM D1044 | 20.0 mg |
| compressive strength | 10%Strain | ASTM D695 | 4.60 Mpa |
| Bending modulus | ASTM D790 | 51.0 Mpa | |
| tensile strength | -- | ASTM D638 | 23.0 Mpa |
| 50%Strain | ASTM D638 | 6.40 Mpa | |
| Physical properties | Test Condition | Test Method | TOYOBO JAPAN/P40UX |
| Shrinkage rate | MD:2.00mm | ASTM D955 | 0.50 % |
| Water absorption rate | Equilibrium,23°C,65%RH | ASTM D570 | 0.48 % |
| melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 10 g/10min |
| thermal performance | Test Condition | Test Method | TOYOBO JAPAN/P40UX |
| Vicat softening temperature | ASTM D1525 | 120 °C | |
| Melting temperature | DSC | 172 °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | <25.0 °C |
| Brittle temperature | JISK6301 | <-65.0 °C | |
| Linear coefficient of thermal expansion | MD | ASTME831 | 1.7E-04 cm/cm/°C |
| Electrical performance | Test Condition | Test Method | TOYOBO JAPAN/P40UX |
| Volume resistivity | ASTM D257 | 2E+12 ohms·cm | |
| Dielectric strength | JISK2111 | 20 KV/mm | |
| flammability | Test Condition | Test Method | TOYOBO JAPAN/P40UX |
| UL flame retardant rating | UL 94 | HB | |
| Supplementary Information | Test Condition | Test Method | TOYOBO JAPAN/P40UX |
| Resilience | JISK6301 | 78 % | |
| hardness | Test Condition | Test Method | TOYOBO JAPAN/P40UX |
| Shore hardness | ShoreA | JISK6301 | 89 |
| ShoreD | ASTM D2240 | 38 |