mechanical propertiesTest ConditionTest MethodSTYRON US/3330
tensile strengthYield,Compression MoldedISO 527-28.34 MPa
Compression Molded,BreakISO 527-217.4 MPa
Yield,Compression MoldedASTMD6388.34 Mpa
Yield,Compression MoldedASTM D-6388.34 MPa
Break,Compression MoldedASTMD63817.4 Mpa
elongationBreak,Compression MoldedASTMD638520 %
tensile strengthCompression Molded,BreakASTM D-63817.4 MPa
Elongation at BreakCompression MoldedASTM D-638520 %
Compression MoldedISO 527-2520 %
Physical propertiesTest ConditionTest MethodSTYRON US/3330
Content of comonomerInternal Method6.5 %
melt mass-flow rate190°C/2.16kgASTMD12385.8 g/10min
thermal performanceTest ConditionTest MethodSTYRON US/3330
Vicat softening temperatureISO 30685
ASTM D-152585
ASTMD152585.0 °C
Melting temperatureInternal Method100 °C
filmTest ConditionTest MethodSTYRON US/3330
Water vapor permeability38°C,90%RHDIN 53122/20.40 g·mm/m²/atm/24hr
Initial sealing temperatureInternal Method92.8 °C
Other performanceTest ConditionTest MethodSTYRON US/3330
Starting temperature of heat sealingInternal Method92.8