| thermal performance | Test Condition | Test Method | STYRON TAIWAN/8701 BK |
|---|---|---|---|
| Vicat softening temperature | -- | ISO 306/B50 | 145 °C |
| Ball pressure temperature | IEC 60335-1 | >130 °C | |
| Vicat softening temperature | -- | ISO 306/A120 | 155 °C |
| Linear coefficient of thermal expansion | MD:-40to80°C | ASTM D696 | 1.5E-05 cm/cm/°C |
| Hot deformation temperature | 1.8MPa,Annealed | ISO 75-2/A | 139 °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 141 °C | |
| 1.8MPa,Unannealed | ISO 75-2/A | 133 °C | |
| Electrical performance | Test Condition | Test Method | STYRON TAIWAN/8701 BK |
| Volume resistivity | 2.00mm | IEC 60093 | 1E+16 ohms·cm |
| Dielectric constant | 2.00mm,1MHz | IEC 60250 | 3.10 |
| Dielectric strength | 2.00mm | IEC 60243-1 | >70 KV/mm |
| Dissipation factor | 2.00mm,50Hz | IEC 60250 | 8E-03 |
| Dielectric constant | 2.00mm,50Hz | IEC 60250 | 3.00 |
| Surface resistivity | IEC 60093 | 1E+14 ohms | |
| Dissipation factor | 2.00mm,1MHz | IEC 60250 | 0.016 |
| impact performance | Test Condition | Test Method | STYRON TAIWAN/8701 BK |
| Impact strength of cantilever beam gap | 23°C,InjectionMolded | ISO 180/A | 9.0 kJ/m² |
| mechanical properties | Test Condition | Test Method | STYRON TAIWAN/8701 BK |
| Bending modulus | 4.00mm,InjectionMolded | ISO 178 | 3800 Mpa |
| Tensile modulus | 4.00mm,InjectionMolded | ISO 527-2/50 | 4000 Mpa |
| tensile strength | Break,4.00mm,Injection | ISO 527-2/50 | 50.0 Mpa |
| bending strength | 4.00mm,InjectionMolded | ISO 178 | 105 Mpa |
| Tensile modulus | 4.00mm,InjectionMolded | ISO 527-2/1 | 3950 Mpa |
| tensile strength | Yield,4.00mm,InjectionMolded | ISO 527-2/50 | 65.0 Mpa |
| Tensile strain | Yield,4.00mm,InjectionMolded | ISO 527-2/50 | 4.0 % |
| Break,4.00mm,Injection | ISO 527-2/50 | 9.0 % | |
| flammability | Test Condition | Test Method | STYRON TAIWAN/8701 BK |
| Extreme Oxygen Index | ISO 4589-2 | 29 % | |
| Hot filament ignition temperature | 3.0mm | IEC 60695-2-13 | 960 °C |
| 2.0mm | IEC 60695-2-13 | 960 °C | |
| UL flame retardant rating | 1.5mm | UL 94 | V-0 |
| Hot filament ignition temperature | 1.0mm | IEC 60695-2-13 | 960 °C |
| Physical properties | Test Condition | Test Method | STYRON TAIWAN/8701 BK |
| Shrinkage rate | MD | ISO 294-4 | 0.40-0.60 % |
| melt mass-flow rate | 300°C/1.2kg | ISO 1133 | 15 g/10min |