PC 8701 BK STYRON TAIWAN
43
Form:Granules | Grade:Injection grade
Properties:
Flame retardantGlass fiber reinforcedenhance
Typical Applications:
InstrumentationVideo devicescomponent
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Instrumentation | Video devices | component |
| Properties: | Flame retardant | Glass fiber reinforced | enhance |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C,InjectionMolded | ISO 180/A | 9.0 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 1.5mm | UL 94 | V-0 | |
| Hot filament ignition temperature | 1.0mm | IEC 60695-2-13 | 960 | °C |
| 2.0mm | IEC 60695-2-13 | 960 | °C | |
| 3.0mm | IEC 60695-2-13 | 960 | °C | |
| Extreme Oxygen Index | ISO 4589-2 | 29 | % | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | 4.00mm,InjectionMolded | ISO 527-2/1 | 3950 | Mpa |
| 4.00mm,InjectionMolded | ISO 527-2/50 | 4000 | Mpa | |
| tensile strength | Yield,4.00mm,InjectionMolded | ISO 527-2/50 | 65.0 | Mpa |
| Break,4.00mm,Injection | ISO 527-2/50 | 50.0 | Mpa | |
| Tensile strain | Yield,4.00mm,InjectionMolded | ISO 527-2/50 | 4.0 | % |
| Break,4.00mm,Injection | ISO 527-2/50 | 9.0 | % | |
| Bending modulus | 4.00mm,InjectionMolded | ISO 178 | 3800 | Mpa |
| bending strength | 4.00mm,InjectionMolded | ISO 178 | 105 | Mpa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 141 | °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 133 | °C | |
| 1.8MPa,Annealed | ISO 75-2/A | 139 | °C | |
| Vicat softening temperature | -- | ISO 306/A120 | 155 | °C |
| -- | ISO 306/B50 | 145 | °C | |
| Ball pressure temperature | IEC 60335-1 | >130 | °C | |
| Linear coefficient of thermal expansion | MD:-40to80°C | ASTM D696 | 1.5E-05 | cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | MD | ISO 294-4 | 0.40-0.60 | % |
| melt mass-flow rate | 300°C/1.2kg | ISO 1133 | 15 | g/10min |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | IEC 60093 | 1E+14 | ohms | |
| Volume resistivity | 2.00mm | IEC 60093 | 1E+16 | ohms·cm |
| Dielectric strength | 2.00mm | IEC 60243-1 | >70 | KV/mm |
| Dielectric constant | 2.00mm,50Hz | IEC 60250 | 3.00 | |
| 2.00mm,1MHz | IEC 60250 | 3.10 | ||
| Dissipation factor | 2.00mm,50Hz | IEC 60250 | 8E-03 | |
| 2.00mm,1MHz | IEC 60250 | 0.016 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.