Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| mechanical properties | Test Condition | Test Method | DSM HOLAND/TW241F3 |
|---|---|---|---|
| tensile strength | Break, 120°C | ISO 527-2 | 85.0 Mpa |
| Break, 180°C | ISO 527-2 | 70.0 Mpa | |
| Break, 160°C | ISO 527-2 | 75.0 Mpa | |
| Tensile strain | Break, 160°C | ISO 527-2 | 12 % |
| Break | ISO 527-2 | 4.0 % | |
| Break, 180°C | ISO 527-2 | 12 % | |
| tensile strength | Break | ISO 527-2 | 140 Mpa |
| Tensile modulus | -- | ISO 527-2 | 6100 Mpa |
| 180°C | ISO 527-2 | 2500 Mpa | |
| 200°C | ISO 527-2 | 2350 Mpa | |
| Bending modulus | ISO 178 | 5800 Mpa | |
| Tensile strain | Break, 120°C | ISO 527-2 | 12 % |
| Tensile modulus | 120°C | ISO 527-2 | 3000 Mpa |
| 160°C | ISO 527-2 | 2650 Mpa | |
| Tensile strain | Break, 200°C | ISO 527-2 | 12 % |
| tensile strength | Break, 200°C | ISO 527-2 | 65.0 Mpa |
| thermal performance | Test Condition | Test Method | DSM HOLAND/TW241F3 |
| Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 290 °C |
| Linear coefficient of thermal expansion | Across Flow | ISO 11359-2 | 8.0E-5 cm/cm/°C |
| Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/A | 275 °C |
| Linear coefficient of thermal expansion | Flow | ISO 11359-2 | 5.0E-5 cm/cm/°C |
| RTI Elec | 0.75 mm | UL 746 | 65.0 °C |
| Melting temperature | ISO 11357-3 | 295 °C | |
| Physical properties | Test Condition | Test Method | DSM HOLAND/TW241F3 |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 3.2 % |
| impact performance | Test Condition | Test Method | DSM HOLAND/TW241F3 |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 50 kJ/m² |
| -30°C | ISO 179/1eU | 45 kJ/m² | |
| flammability | Test Condition | Test Method | DSM HOLAND/TW241F3 |
| Flammability level | UL 94 | HB |