impact performanceTest ConditionTest MethodBASF GERMANY/796M
Impact strength of cantilever beam gap-30°CISO 180/A5.0 kJ/m²
Charpy Notched Impact Strength23°CISO 17930 kJ/m²
Impact strength of cantilever beam gap23°CISO 180/A25 kJ/m²
Charpy Notched Impact Strength-30°CISO 1795.0 kJ/m²
mechanical propertiesTest ConditionTest MethodBASF GERMANY/796M
bending strengthISO 17860.0 Mpa
tensile strengthYield,23°CISO 527-241.0 Mpa
Tensile strainYield,23°CISO 527-23.5 %
Tensile modulusISO 527-22000 Mpa
Electrical performanceTest ConditionTest MethodBASF GERMANY/796M
Volume resistivityIEC 600931E+14 ohms·cm
Dielectric constant100HzIEC 602503.80
Dissipation factor1MHzIEC 602500.025
Surface resistivityIEC 600931E+13 ohms
Dissipation factor100HzIEC 602500.010
Physical propertiesTest ConditionTest MethodBASF GERMANY/796M
densityISO 11831.07 g/cm³
Melt Volume Flow Rate (MVR)220°C/10.0kgISO 11339.00 cm3/10min
Water absorption rateEquilibrium,23°C,50%RHISO 620.35 %
Shrinkage rateISO 294-40.50-0.90 %
Water absorption rateSaturation,23°CISO 621.7 %
hardnessTest ConditionTest MethodBASF GERMANY/796M
Ball Pressure TestISO 2039-165.0 Mpa
filmTest ConditionTest MethodBASF GERMANY/796M
elongationBreak13 %
thermal performanceTest ConditionTest MethodBASF GERMANY/796M
0.45MPa, annealedISO 75-2/B100 °C
Linear coefficient of thermal expansionMDISO 11359-28.0E-5到1.1E-4 cm/cm/°C
1.8MPa, annealedISO 75-2/A95.0 °C
thermal conductivityDIN 526120.17 W/m/K