Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| optical performance | Test Condition | Test Method | SUMITOMO JAPAN/SD2201W |
|---|---|---|---|
| turbidity | 2000 μm2000 μm | JIS K7136 | 0.3 % |
| Transmittance rate | 2000 μm2000 μm | JIS K7361 | 90.6 % |
| mechanical properties | Test Condition | Test Method | SUMITOMO JAPAN/SD2201W |
| bending strength | ISO 178 | 80 Mpa | |
| Bending modulus | ISO 178 | 2200 Mpa | |
| Tensile modulus | ISO 527-2 | 2000 Mpa | |
| tensile strength | ISO 527-2 | 64 Mpa | |
| Tensile strain | BreakBreak | ISO 527-2 | 50 % |
| flame retardant performance | Test Condition | Test Method | SUMITOMO JAPAN/SD2201W |
| UL flame retardant rating | 3.00 mm | V-2 | |
| 0.40 mm | V-2 | ||
| thermal performance | Test Condition | Test Method | SUMITOMO JAPAN/SD2201W |
| Hot deformation temperature | 1.8 MPa,Unannealed1.8 MPa,Unannealed | ISO 75-2/A | 122 °C |
| Physical properties | Test Condition | Test Method | SUMITOMO JAPAN/SD2201W |
| density | ISO 1183 | 1.2 g/cm³ | |
| impact performance | Test Condition | Test Method | SUMITOMO JAPAN/SD2201W |
| Charpy Notched Impact Strength | 23℃23℃ | ISO 179 | 5 kJ/m² |