Product Description
Certificates(0)
Datasheet
Product Description
Certificates
No Data...
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| turbidity | 2000 μm2000 μm | JIS K7136 | 0.3 | % |
| Transmittance rate | 2000 μm2000 μm | JIS K7361 | 90.6 | % |
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
| Charpy Notched Impact Strength | 23℃23℃ | ISO 179 | 5 | kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | ISO 178 | 80 | Mpa | |
| Bending modulus | ISO 178 | 2200 | Mpa | |
| Tensile strain | BreakBreak | ISO 527-2 | 50 | % |
| tensile strength | ISO 527-2 | 64 | Mpa | |
| Tensile modulus | ISO 527-2 | 2000 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8 MPa,Unannealed1.8 MPa,Unannealed | ISO 75-2/A | 122 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ISO 1183 | 1.2 | g/cm³ | |
| flame retardant performance | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 3.00 mm | V-2 | ||
| 0.40 mm | V-2 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.