| mechanical properties | Test Condition | Test Method | KUMHO KOREA/HW600G |
|---|---|---|---|
| elongation | Break | ASTM D638 | 22 % |
| bending strength | --2 | ISO 178 | 65.0 Mpa |
| Bending modulus | --2 | ISO 178 | 2300 Mpa |
| bending strength | -- | ASTM D790 | 72.0 Mpa |
| elongation | Break | ISO 527-2/50 | 25 % |
| Bending modulus | -- | ASTM D790 | 2200 Mpa |
| tensile strength | -- | ISO 527-2/50 | 47.0 Mpa |
| -- | ASTM D638 | 52.0 Mpa | |
| thermal performance | Test Condition | Test Method | KUMHO KOREA/HW600G |
| Vicat softening temperature | -- | ISO 306/B50 | 96.0 °C |
| Hot deformation temperature | 1.8MPa,Unannealed5 | ISO 75-2/A | 78.0 °C |
| 1.8MPa,Unannealed | ASTM D648 | 85.0 °C | |
| Vicat softening temperature | -- | ASTM D15256 | 95.0 °C |
| Electrical performance | Test Condition | Test Method | KUMHO KOREA/HW600G |
| Volume resistivity | IEC 60093 | >1.0E+15 ohms·cm | |
| Surface resistivity | IEC 60093 | >1.0E+15 ohms | |
| impact performance | Test Condition | Test Method | KUMHO KOREA/HW600G |
| Charpy Notched Impact Strength | 23°C | ISO 179 | 15 kJ/m² |
| Impact strength of simply supported beam without notch | 23°C | ISO 179 | 60 kJ/m² |
| Charpy Notched Impact Strength | -30°C | ISO 179 | 7.0 kJ/m² |
| flammability | Test Condition | Test Method | KUMHO KOREA/HW600G |
| UL flame retardant rating | UL 94 | HB | |
| Physical properties | Test Condition | Test Method | KUMHO KOREA/HW600G |
| Shrinkage rate | MD | ASTM D955 | 0.40-0.70 % |
| -- | ISO 294-4 | 0.40-0.70 % | |
| melt mass-flow rate | 220°C/10.0kg | ISO 1133 | 24 g/10min |
| 220°C/10.0kg | ASTM D1238 | 17 g/10min |