| mechanical properties | Test Condition | Test Method | BASF GERMANY/N2200G53UN |
|---|---|---|---|
| Tensile stress | 73℉,Break | ISO 527-1 | 18900 psi |
| Charpy Notched Impact Strength | 73℉ | ISO 179 | 4.28 ft·lb/in |
| Tensile strain | 73℉,Break | ISO 527-1 | 3.0 % |
| Impact strength of simply supported beam without notch | -22℉ | ISO 179 | 28.6 ft·lb/in |
| Tensile creep modulus | 1000h | ISO 899-1 | 841000 psi |
| Charpy Notched Impact Strength | -22℉ | ISO 179 | 4.04 ft·lb/in |
| Impact strength of simply supported beam without notch | 73℉ | ISO 179 | 26.2 ft·lb/in |
| Tensile modulus | 73℉ | ISO 527-1 | 1.28E+06 psi |
| Electrical performance | Test Condition | Test Method | BASF GERMANY/N2200G53UN |
| Volume resistivity | IEC 60093 | 1E+14 ohm·cm | |
| Dielectric loss | 1E+6HZ,73℉ | IEC 60250 | 0.00700 |
| Surface resistivity | IEC 60093 | 1E+14 ohms | |
| Physical properties | Test Condition | Test Method | BASF GERMANY/N2200G53UN |
| density | ISO 1183 | 1.58 | |
| Water absorption rate | 23C/50RH | ISO 62 | 0.15 % |
| thermal performance | Test Condition | Test Method | BASF GERMANY/N2200G53UN |
| Hot deformation temperature | 1.80MPa | ISO 75A-1 | 325 ℉ |
| UL flame retardant rating | UL 94 | HB |