POM N2200G53UN BASF GERMANY
180
Form:Granules | Grade:Injection grade
Properties:
High toughness25% glass fiber reinforce
Typical Applications:
ToyAutomotive Applications
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Toy | Automotive Applications |
| Properties: | High toughness | 25% glass fiber reinforce |
Certificates

Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of simply supported beam without notch | 73℉ | ISO 179 | 26.2 | ft·lb/in |
| -22℉ | ISO 179 | 28.6 | ft·lb/in | |
| Charpy Notched Impact Strength | 73℉ | ISO 179 | 4.28 | ft·lb/in |
| -22℉ | ISO 179 | 4.04 | ft·lb/in | |
| Tensile creep modulus | 1000h | ISO 899-1 | 841000 | psi |
| Tensile strain | 73℉,Break | ISO 527-1 | 3.0 | % |
| Tensile stress | 73℉,Break | ISO 527-1 | 18900 | psi |
| Tensile modulus | 73℉ | ISO 527-1 | 1.28E+06 | psi |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | UL 94 | HB | ||
| Hot deformation temperature | 1.80MPa | ISO 75A-1 | 325 | ℉ |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | 23C/50RH | ISO 62 | 0.15 | % |
| density | ISO 1183 | 1.58 | ||
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric loss | 1E+6HZ,73℉ | IEC 60250 | 0.00700 | |
| Volume resistivity | IEC 60093 | 1E+14 | ohm·cm | |
| Surface resistivity | IEC 60093 | 1E+14 | ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.