Material Comparison
Add Comparison Model
Highlight Differences
Hide Same

Product Name Manufacturer Model

Brand

Typical Applications

Properties

Color

Form

Processing Methods

Grade

Filler

Recycled Content

Certificates

Reference Price

thermal performanceTest ConditionTest MethodDSM HOLAND/TS350 NA
Linear coefficient of thermal expansionAcross FlowISO 11359-29.0E-5 cm/cm/°C
Hot deformation temperature1.8 MPa, UnannealedISO 75-2/A190 °C
Linear coefficient of thermal expansionFlowISO 11359-28.0E-5 cm/cm/°C
Melting temperatureISO 11357-3295 °C
impact performanceTest ConditionTest MethodDSM HOLAND/TS350 NA
Charpy Notched Impact Strength23°CISO 179/1eA4.0 kJ/m²
-30°CISO 179/1eA3.0 kJ/m²
Electrical performanceTest ConditionTest MethodDSM HOLAND/TS350 NA
Volume resistivityIEC 600931.0E+15 ohms·cm
Relative permittivity100 HzIEC 602503.80
1 MHzIEC 602503.50
Dielectric strengthIEC 60243-130 KV/mm
Physical propertiesTest ConditionTest MethodDSM HOLAND/TS350 NA
densityISO 11831.43 g/cm³
Water absorption rateEquilibrium, 23°C, 50% RHISO 622.4 %
Shrinkage rateFlowISO 294-41.5 %
横向FlowISO 294-41.5 %
mechanical propertiesTest ConditionTest MethodDSM HOLAND/TS350 NA
Nominal tensile fracture strainISO 527-27.0 %
tensile strengthYieldISO 527-280.0 Mpa
Bending modulusISO 1783200 Mpa
Tensile modulusISO 527-23400 Mpa
flammabilityTest ConditionTest MethodDSM HOLAND/TS350 NA
Flammability levelUL 94V-0