Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Certificates
Reference Price
| Supplementary Information | Test Condition | Test Method | DUPONT USA/LW9320 |
|---|---|---|---|
| Odor | VDA270 | 3.50 | |
| EmissionofOrganicCompounds | VDA277 | 130 µgC/g | |
| thermal performance | Test Condition | Test Method | DUPONT USA/LW9320 |
| Melting temperature | ISO 3146 | 220 ℃ | |
| UL flame retardant rating | 0.750 mm | UL94 | HB |
| Hot deformation temperature | 1.80 Mpa,Unannealed | ISO 75A-1 | 180 ℃ |
| 1.8MPa,Unannealed | ISO 75-2/A | 175 °C | |
| Melting temperature | ISO 11357-3 | 220 °C | |
| UL flame retardant rating | 3.00 mm | UL94 | HB |
| 1.50 mm | UL94 | HB | |
| Linear coefficient of thermal expansion | MD | ISO 11359-2 | 3E-05 cm/cm/°C |
| Glass transition temperature | ISO 11357-2 | 110 °C | |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 1E-04 cm/cm/°C |
| flammability | Test Condition | Test Method | DUPONT USA/LW9320 |
| UL flame retardant rating | 1.5mm | IEC 60695-11-10,-20 | HB |
| 1.5mm | UL 94 | HB | |
| 0.75mm | IEC 60695-11-10,-20 | HB | |
| 0.75mm | UL 94 | HB | |
| Burning rate | 1.00mm | ISO 3795 | 30 mm/min |
| FMVSS flammability | FMVSS302 | B | |
| Physical properties | Test Condition | Test Method | DUPONT USA/LW9320 |
| density | ISO 1183 | 1.35 g/cm³ | |
| Shrinkage rate | MD | ISO 294-4 | 0.40 % |
| Top out temperature | 170 °C | ||
| SpecificHeatCapacity of Melt | 1900 J/kg/°C | ||
| Shrinkage rate | TD | ISO 294-4 | 0.70 % |
| MediumDensity | 1.17 g/cm³ | ||
| Shrinkage rate | Flow | ISO 294-4 | 0.4 % |
| Melt Volume Flow Rate (MVR) | 250°C/5.0kg | ISO 1133 | 15.0 cm3/10min |
| Shrinkage rate | Across Flow | ISO 294-4 | 0.65 % |
| Water absorption rate | Equilibrium,23°C,2.00mm,50%RH | ISO 62 | 0.30 % |
| ThermalConductivityofMelt | 0.24 W/m/K | ||
| Stickiness | ISO 307 | 120 cm³/g | |
| impact performance | Test Condition | Test Method | DUPONT USA/LW9320 |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 45 kJ/m² |
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 8.0 kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 7.0 kJ/m² |
| -40°C | ISO 180/1A | 7.0 kJ/m² | |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 50 kJ/m² |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 8.5 kJ/m² |
| Impact strength of cantilever beam gap | -30°C | ISO 180/1A | 7.0 kJ/m² |
| mechanical properties | Test Condition | Test Method | DUPONT USA/LW9320 |
| Tensile strain | Break | ISO 527-2 | 2.5 % |
| Tensile modulus | ISO 527-2 | 7500 Mpa | |
| 23℃ | ISO 527-1 | 7400 MPa | |
| Tensile stress | 23℃,Break | ISO 527-1 | 120 MPa |
| Impact strength of cantilever beam gap | -40 ℃, Type 1, Notch A | ISO 180 | 7 KJ/m |
| Bending modulus | ISO 178 | 7000 Mpa | |
| Impact strength of simply supported beam without notch | 23 ℃, Type 1, Edgewise | ISO 179 | 55 KJ/m |
| tensile strength | Break | ISO 527-2 | 120 Mpa |
| Tensile strain | Break | ISO 527-1 | 2.7 % |
| Bending modulus | 23℃ | ISO 178 | 6100 MPa |
| Charpy Notched Impact Strength | 23 °C, Type 1, Edgewise, Notch A | ISO 179 | 8.5 KJ/m |
| Impact strength of cantilever beam gap | 23 ℃, Type 1, Notch A | ISO 180 | 7 KJ/m |