| thermal performance | Test Condition | Test Method | COVESTRO SHANGHAI/FR3023 901510 |
|---|---|---|---|
| Vicat softening temperature | -- | ISO 306/B50 | 99.0 °C |
| Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 96.0 °C |
| 1.8 MPa, Unannealed | ISO 75-2/A | 88.0 °C | |
| Vicat softening temperature | -- | ISO 306/B120 | 102 °C |
| flammability | Test Condition | Test Method | COVESTRO SHANGHAI/FR3023 901510 |
| UL flame retardant rating | 1.2 mm | UL 94 | V-0 |
| Burning wire flammability index | 1.0 mm | IEC 60695-2-12 | 850 °C |
| Physical properties | Test Condition | Test Method | COVESTRO SHANGHAI/FR3023 901510 |
| Shrinkage rate | Flow | ISO 2577 | 0.20 - 0.30 % |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 0.20 % |
| Saturation, 23°C | ISO 62 | 0.50 % | |
| Melt Volume Flow Rate (MVR) | 260°C/5.0 kg | ISO 1133 | 24.0 cm3/10min |
| Shrinkage rate | 横向Flow | ISO 2577 | 0.20 - 0.30 % |
| mechanical properties | Test Condition | Test Method | COVESTRO SHANGHAI/FR3023 901510 |
| Tensile strain | Yield, 23°C | ISO 527-2/50 | 3.2 % |
| Tensile modulus | 23°C | ISO 527-2/1 | 5400 Mpa |
| tensile strength | Yield, 23°C | ISO 527-2/50 | 62.0 Mpa |
| Break, 23°C | ISO 527-2/50 | 48.0 Mpa | |
| Tensile strain | Break, 23°C | ISO 527-2/50 | 6.0 % |
| impact performance | Test Condition | Test Method | COVESTRO SHANGHAI/FR3023 901510 |
| Suspended wall beam without notch impact strength | 23°C | ISO 180 | 52 kJ/m² |
| Electrical performance | Test Condition | Test Method | COVESTRO SHANGHAI/FR3023 901510 |
| Volume resistivity | 23°C | IEC 60093 | 1.0E+17 ohms·cm |
| Surface resistivity | IEC 60093 | 1.0E+16 ohms | |
| Filling analysis | Test Condition | Test Method | COVESTRO SHANGHAI/FR3023 901510 |
| Melt viscosity | 260°C | ISO 11443-A | 220 Pa·s |