Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Certificates
Reference Price
| Basic Performance | Test Condition | Test Method | KOTEC JAPAN/K-30 |
|---|---|---|---|
| melt mass-flow rate | 300℃,1.2kg | ASTM D-1238 | 15.0 g/10min |
| mechanical properties | Test Condition | Test Method | KOTEC JAPAN/K-30 |
| elongation | Break | ASTM D-638 | 120 % |
| Elongation at Break | ASTM D638/ISO 527 | 120 % | |
| Impact strength of cantilever beam gap | ASTM D256/ISO 179 | 80 kg·cm/cm(J/M)ft·lb/in | |
| Rockwell hardness | ASTM D785 | 115 | |
| Impact strength of cantilever beam gap | 23℃,VNotched,1/8" | ASTM D-256 | 14.3 Kgf.cm/cm |
| bending strength | ASTM D-790 | 85 Ibf/in | |
| tensile strength | ASTM D638/ISO 527 | (62) kg/cm²(MPa)[Lb/in²] | |
| bending strength | ASTM D790/ISO 178 | (85) kg/cm²(MPa)[Lb/in²] | |
| Bending modulus | ASTM D-790 | 22000 Ibf/in | |
| tensile strength | ASTM D-638 | 9100 Kgf/cm | |
| other | Test Condition | Test Method | KOTEC JAPAN/K-30 |
| purpose | 注塑.薄成型.一般用途 | ||
| characteristic | 分别为低粘度.高流量/低粘度/中粘度品级 | ||
| Color | 透明 | ||
| thermal performance | Test Condition | Test Method | KOTEC JAPAN/K-30 |
| Hot deformation temperature | HDT | ASTM D648/ISO 75 | 133 ℃(℉) |
| UL flame retardant rating | UL -94 | V-2 | |
| Hot deformation temperature | 18.6Kg/cm | ASTM D-648 | 133 °C |
| Electrical performance | Test Condition | Test Method | KOTEC JAPAN/K-30 |
| Volume resistivity | ASTM D257/IEC 60093 | 10^16 Ω.cm | |
| ASTM D-257 | 10 Ω.cm | ||
| Physical properties | Test Condition | Test Method | KOTEC JAPAN/K-30 |
| density | ASTM D792/ISO 1183 | 1.2 |