| mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE SAUDI/HCPO-CX02 82 00900 |
|---|---|---|---|
| Impact strength of cantilever beam gap | 0℃ | ISO 180/4A | 6.0 KJ/m |
| Charpy Notched Impact Strength | 23℃ | ISO 179/1eA | 7.0 KJ/m |
| Shore hardness | ISO 868 | 70 | |
| tensile strength | Break | ISO 527 | 24 Mpa |
| elongation | Break | ISO 527 | 600 % |
| Impact strength of cantilever beam gap | -20℃ | ISO 180/4A | 4.5 KJ/m |
| 23℃ | ISO 180/4A | 8.5 KJ/m | |
| tensile strength | Yield | ISO 527 | 30 Mpa |
| Bending modulus | ASTM D-790 | 1700 Mpa | |
| thermal performance | Test Condition | Test Method | SABIC INNOVATIVE SAUDI/HCPO-CX02 82 00900 |
| Hot deformation temperature | 0.45MPa (HDT/B) | ISO 75/B | 105 °C |
| Vicat softening temperature | 10N (VST/A) | ISO 306/A | 145 °C |
| Linear coefficient of thermal expansion | -30℃~30℃ | ASTM D-696 | 120 µm/mK |
| Basic Performance | Test Condition | Test Method | SABIC INNOVATIVE SAUDI/HCPO-CX02 82 00900 |
| melt mass-flow rate | 230℃,2.16kg | ISO 1133 | 15 g/10min |
| Shrinkage rate | SABIC method | 1.6 % | |
| density | ISO 1183 | 0.905 |