| thermal performance | Test Condition | Test Method | JILIN JOINATURE/550CA20 |
|---|---|---|---|
| Hot deformation temperature | 1.8 Mpa | ISO 75-f | 325 °C |
| thermal conductivity | 23℃ | ISO 22007-4 | 0.95 W/m/K |
| Linear coefficient of thermal expansion | 低于Tg沿着Flow | ISO 11359 | 8 ppm/K |
| specific heat | 23℃ | DSC | 1.8 kJ/kg/℃ |
| Melting temperature | ISO 11357 | 343 °C | |
| Linear coefficient of thermal expansion | 高于Tg沿着Flow | ISO 11359 | 8 ppm/K |
| Glass transition temperature | 起始 | ISO 11357 | 143 °C |
| impact performance | Test Condition | Test Method | JILIN JOINATURE/550CA20 |
| Impact strength of cantilever beam gap | 有Notched | ISO 180-A | 8 kJ/m² |
| ISO 180/U | 40 kJ/m² | ||
| Charpy Notched Impact Strength | ISO 179/1U | 45 kJ/m² | |
| ISO 179/1eA | 7 kJ/m² | ||
| Physical properties | Test Condition | Test Method | JILIN JOINATURE/550CA20 |
| Water absorption rate | 23℃,24hr,3.20 mm | ISO 62-1 | 0.05 % |
| Shrinkage rate | MD | ISO 294-4 | 0.7 % |
| TD | ISO 294-4 | 0.2 % | |
| melt mass-flow rate | 380℃,5.0kg | ISO 1133 | 7 g/10min |
| density | 结晶 | ISO 1183 | 1.37 g/cm³ |
| Water absorption rate | Equilibrium,23℃,3.20 mm | ISO 62-1 | 0.4 % |
| mechanical properties | Test Condition | Test Method | JILIN JOINATURE/550CA20 |
| Tensile strain | Break,23℃ | ISO 527 | 2 % |
| bending strength | Break,23℃ | ISO 178 | 310 Mpa |
| Shore hardness | 23℃ | ISO 868 | 86 D 级 |
| Bending modulus | 23℃ | ISO 178 | 16000 Mpa |
| tensile strength | Break,23℃ | ISO 527 | 205 Mpa |
| Electrical performance | Test Condition | Test Method | JILIN JOINATURE/550CA20 |
| Volume resistivity | 23 ℃,1V | IEC 60093 | 10^7 ohms·cm |