Material Description
- Material Properties:Conductive|High rigidity|high strength|Halogen-free|Flame retardant|Carbon fiber reinforced|Special strength and stiffness|30% carbon fiber reinforcement|Conductive|Special strength and stiffness|30% carbon fiber reinforcement|Conductive
- Application Areas:Metal substitution
- Color:--
- Grade:Conductive grade
Technical Data Sheet
| Basic Performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | ISO 1183 | 1500 kg/m |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | ISO 527-1 | 200 Mpa | |
| elongation | Break | ISO 527-1 | 0.70 % |
| Bending modulus | 23℃ | ISO 178 | 25500 Mpa |
| bending strength | 23℃ | ISO 178 | 320 Mpa |
| Charpy Notched Impact Strength | 23℃ | ISO 179/1eA | 6.00 KJ/m |
| Impact strength of simply supported beam without notch | 23℃ | ISO 179/1eU | 15.0 KJ/m |
| Impact strength of cantilever beam gap | 23℃ | ISO 180/1A | 10.00 KJ/m |
| Suspended wall beam without notch impact strength | 23℃ | ISO 180/1U | 12.0 KJ/m |
| Rockwell hardness | ISO 2039-2 | 99 M Scale | |
| Tensile modulus | ISO 527-1 | 31800 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa | ISO 75-1 | 250 °C |
| 1.80MPa | ISO 75-1 | 235 °C | |
| 8.00MPa | ISO 75-1 | 186 °C | |
| Vicat softening temperature | 50℃/h 50N | ISO 306 | 167 °C |
| Crystallization peak temperature | ISO 11357-1 | 280 °C | |
| Linear coefficient of thermal expansion | parallel | ISO 11359-1 | 1E-06 cm/cm℃ |
| normal | ISO 11359-1 | 4E-06 cm/cm℃ | |
| Combustibility | UL 94 | V-0 |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shrinkage rate | normal | ISO 2577 | 0.0 % |
| parallel | ISO 2577 | 0.10 % |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Surface resistivity | IEC 60093 | 1E+02 ohms | |
| Volume resistivity | IEC 60093 | 0.10 ohm.m | |
| Relative permittivity | 1000Hz | IEC 60250 | 32.0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.