TPEE BEXLOY® 4053FG NC010 DUPONT LUXEMBOURG
220
- Unit Price:US$ 7,343 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:Thermal stability|Aging resistance|UV resistance
- Application Areas:Automotive Applications|Fitness equipment|electrical equipment|Non specific food applications
- Color:--
- Grade:--
Technical Data Sheet
impact performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ISO 8256/1 | 230 kJ/m² |
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | NoBreak |
23°C | ISO 179/1eU | NoBreak |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | 1.5mm | UL 94 | HB |
Flammability level | 1.5mm | IEC 60695-11-10,-20 | HB |
Extreme Oxygen Index | ISO 4589-2 | 20 % | |
FMVSS flammability | FMVSS302 | SE |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
tear strength | Flow | ISO 34-1 | 110 kN/m |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | 10%Strain | ISO 527-2 | 4.10 Mpa |
50%Strain | ISO 527-2 | 7.30 Mpa | |
Tensile modulus | ISO 527-2 | 56.0 Mpa | |
tensile strength | Break | ISO 527-2 | 26.0 Mpa |
5.0%Strain | ISO 527-2 | 2.40 Mpa | |
Tensile strain | Break | ISO 527-2 | >300 % |
Tensile creep modulus | 1hr | ISO 899-1 | 50.0 Mpa |
1000hr | ISO 899-1 | 40.0 Mpa |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Glass transition temperature | ISO 11357-2 | -50.0 °C | |
Melting temperature | ISO 11357-3 | 150 °C | |
Linear coefficient of thermal expansion | MD | ISO 11359-2 | 2.2E-04 cm/cm/°C |
TD | ISO 11359-2 | 2.2E-04 cm/cm/°C | |
Effective thermal diffusivity coefficient | 5.44E-08 m²/s |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 5.3 g/10min |
Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 5.00 cm3/10min |
Shrinkage rate | TD | ISO 294-4 | 0.40 % |
MD | ISO 294-4 | 0.20 % | |
Water absorption rate | Saturation,23°C,2.00mm | ISO 62 | 0.70 % |
Equilibrium,23°C,2.00mm,50%RH | ISO 62 | 0.20 % | |
MediumDensity | 1.02 g/cm³ |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Relative permittivity | 100Hz | IEC 60250 | 5.20 |
1MHz | IEC 60250 | 4.70 | |
Dissipation factor | 100Hz | IEC 60250 | 0.011 |
1MHz | IEC 60250 | 0.053 | |
Compared to the anti leakage trace index | IEC 60112 | PLC 0 | |
Surface resistivity | IEC 60093 | 2E+14 ohms | |
Volume resistivity | IEC 60093 | 7E+12 ohms·cm | |
Dielectric strength | IEC 60243-1 | 18 KV/mm |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore hardness | ShoreD,15Sec | ISO 868 | 38 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.