PA66 TECHNYL® A 205F SOLVAY FRANCE
316
- Unit Price:US$ 3,128 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:45MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:--
- Application Areas:Thin walled components|Fasteners|Laptop case
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183/A | 1.14 g/cm³ | |
Water absorption rate | ISO 62 | 1.2 % |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL 94 | V-2 | |
UL 94 | V-2 | ||
UL 94 | V-2 | ||
UL 94 | V-2 | ||
Burning wire flammability index | IEC 60695-2-12 | 850 °C | |
Limiting Oxygen Index | ISO 4589-2 | 29 % | |
UL flame retardant rating | NFF16-101 | F2 | |
smoke density | NFF16-101 | I3 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
EuropeanRailwaysCertifications | EN45545-2 | HL2 | |
EN45545-2 | HL2 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ISO 527-2/1A | 3200 Mpa | |
tensile strength | ASTM D638 | 85.0 Mpa | |
ISO 527-2/1A | 85.0 Mpa | ||
ISO 527-2/1A | 60.0 Mpa | ||
Tensile strain | ISO 527-2 | 4.0 % | |
elongation | ASTM D638 | 25 % | |
Tensile strain | ISO 527-2 | 50 % | |
Flexural modulus | ASTM D790 | 3350 Mpa | |
ISO 178 | 3000 Mpa | ||
bending strength | ASTM D790 | 125 Mpa | |
ISO 178 | 120 Mpa |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | 5.0 kJ/m² | |
Impact strength of simply supported beam without notch | ISO 179/1eU | NoBreak | |
Impact strength of cantilever beam gap | ASTM D256 | 80 J/m | |
ISO 180 | 5.0 kJ/m² |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface Resistivity | IEC 60093 | 5E+15 ohms | |
Volume resistivity | IEC 60093 | 1E+15 ohms·cm | |
dielectric strength | IEC 60243-1 | 27 KV/mm | |
relative permittivity | IEC 60250 | 2.90 | |
Dissipation Factor | IEC 60250 | 0.030 | |
Compared to the Leakage Tracking Index (CTI) | IEC 60112 | PLC 0 | |
IEC 60112 | PLC 1 |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ISO 75-2/Bf | 205 °C | |
ASTM D648 | 80.0 °C | ||
ISO 75-2/Af | 65.0 °C | ||
melting temperature | ISO 11357-3 | 263 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.