POM TENAC™ MG210 ASAHI JAPAN
250
- Unit Price:US$ 5,615 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:high viscosity|High toughness|Fatigue resistance|Creep resistance|High impact resistance|high strength|High rigidity|Dimensional stability
- Application Areas:Engine parts|Engineering accessories|Shell|Conveyor accessories|Fasteners|Automotive sector|bearing|Engineering accessories|Engine parts|Fasteners|Shell|bearing|Conveyor accessories|Application in the automotive field
- Color:--
- Grade:Injection grade
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Taber abraser | ASTM D1044 | 13.0 mg | |
| bending strength | ASTM D790 | 108 Mpa | |
| Bending modulus | -- | ISO 178 | 2900 Mpa |
| -- | ASTM D790 | 3040 Mpa | |
| elongation | Break | ASTMD638 | 40 % |
| tensile strength | -- | ASTM D638 | 79.0 Mpa |
| Yield | ISO 527-2 | 75.0 Mpa | |
| Tensile modulus | ISO 527-2 | 3150 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 136 °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 103 °C | |
| 0.45MPa,Unannealed | ISO 75-2/B | 167 °C | |
| 0.45MPa,Unannealed | ASTM D648 | 172 °C | |
| thermal conductivity | 0.23 W/m/K | ||
| specific heat | 1470 J/kg/°C | ||
| Linear coefficient of thermal expansion | MD | ASTMD696 | 1E-04 cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Water absorption rate | 23°C,24hr,50%RH | ASTM D570 | 0.20 % |
| Shrinkage rate | MD | Internal Method | 1.8-2.2 % |
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 1.7 g/10min |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Volume resistivity | 23°C | ASTM D257 | 1.0E+15-1.0E+16 ohms·cm |
| Surface resistivity | ASTM D257 | 1.0E+16-1.0E+17 ohms | |
| Arc resistance | ASTM D495 | 250 sec | |
| Dissipation factor | 23°C,1MHz | ASTM D150 | 7E-03 |
| Dielectric constant | 23°C,1MHz | ASTM D150 | 3.80 |
| Dielectric strength | ASTM D149 | 18 KV/mm |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Rockwell hardness | R-Scale | ASTM D785 | 120 |
| M-Scale | ASTM D785 | 94 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.