Material Description
- Material Properties:Thermal stability|enhance|Filler: Glass fiber reinforced material|35% filler by weight
- Application Areas:Electronic and Electrical Applications
- Color:--
- Grade:--
Technical Data Sheet
impact performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 75 kJ/m² |
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 12 kJ/m² |
-40°C | ISO 179/1eA | 9.0 kJ/m² |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
FMVSS flammability | FMVSS302 | SE |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Poisson's ratio | ISO 527 | 0.38 | |
Bending modulus | ISO 178 | 9000 Mpa | |
Tensile creep modulus | 1000hr | ISO 899-1 | -- Mpa |
1hr | ISO 899-1 | -- Mpa | |
Tensile strain | Break | ISO 527-2 | 3.0 % |
tensile strength | Break | ISO 527-2 | 180 Mpa |
Tensile modulus | ISO 527-2 | 10000 Mpa |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Linear coefficient of thermal expansion | TD:-40to23°C | ISO 11359-2 | 7.5E-05 cm/cm/°C |
TD:-- | ISO 11359-2 | 7.2E-05 cm/cm/°C | |
MD:-40to23°C | ISO 11359-2 | 2E-05 cm/cm/°C | |
MD:-- | ISO 11359-2 | 2E-05 cm/cm/°C | |
Melting temperature | ISO 11357-3 | 300 °C | |
Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 255 °C |
0.45MPa,Unannealed | ISO 75-2/B | 285 °C | |
Linear coefficient of thermal expansion | TD:导热系数 | ISO 11359-2 | 0.35 W/m/K |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Shrinkage rate | MD | ISO 294-4 | 0.20 % |
TD | ISO 294-4 | 0.60 % | |
density | ISO 1183 | 1.42 g/cm³ |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Compared to the anti leakage trace index | IEC 60112 | PLC 0 | |
Dielectric strength | IEC 60243-1 | 43 KV/mm | |
Surface resistivity | IEC 60093 | -- ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.