Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Reference Price
| mechanical properties | Test Condition | Test Method | DUPONT USA/HTN54G35HSLR NC010 |
|---|---|---|---|
| Tensile creep modulus | 1hr | ISO 899-1 | -- Mpa |
| Poisson's ratio | ISO 527 | 0.38 | |
| Tensile strain | Break | ISO 527-2 | 3.0 % |
| tensile strength | Break | ISO 527-2 | 180 Mpa |
| Tensile modulus | ISO 527-2 | 10000 Mpa | |
| Bending modulus | ISO 178 | 9000 Mpa | |
| Tensile creep modulus | 1000hr | ISO 899-1 | -- Mpa |
| impact performance | Test Condition | Test Method | DUPONT USA/HTN54G35HSLR NC010 |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 75 kJ/m² |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 12 kJ/m² |
| -40°C | ISO 179/1eA | 9.0 kJ/m² | |
| thermal performance | Test Condition | Test Method | DUPONT USA/HTN54G35HSLR NC010 |
| Linear coefficient of thermal expansion | MD:-40to23°C | ISO 11359-2 | 2E-05 cm/cm/°C |
| MD:-- | ISO 11359-2 | 2E-05 cm/cm/°C | |
| TD:导热系数 | ISO 11359-2 | 0.35 W/m/K | |
| TD:-- | ISO 11359-2 | 7.2E-05 cm/cm/°C | |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 285 °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 255 °C | |
| Linear coefficient of thermal expansion | TD:-40to23°C | ISO 11359-2 | 7.5E-05 cm/cm/°C |
| Melting temperature | ISO 11357-3 | 300 °C | |
| Physical properties | Test Condition | Test Method | DUPONT USA/HTN54G35HSLR NC010 |
| density | ISO 1183 | 1.42 g/cm³ | |
| Shrinkage rate | MD | ISO 294-4 | 0.20 % |
| TD | ISO 294-4 | 0.60 % | |
| flammability | Test Condition | Test Method | DUPONT USA/HTN54G35HSLR NC010 |
| FMVSS flammability | FMVSS302 | SE | |
| Electrical performance | Test Condition | Test Method | DUPONT USA/HTN54G35HSLR NC010 |
| Compared to the anti leakage trace index | IEC 60112 | PLC 0 | |
| Surface resistivity | IEC 60093 | -- ohms | |
| Dielectric strength | IEC 60243-1 | 43 KV/mm |