Material Description
- Material Properties:Toughening|High impact resistance
- Application Areas:film
- Color:--
- Grade:Halogen-free flame retardant grade
Technical Data Sheet
| Other performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| tensile strength | @100% Elongation | ASTM D-412 | 407(2.8) | Psi(MPa) |
| Elongation at Break | @Break | ASTM D-412 | No Break | % |
| tensile strength | ASTM D-624 | 245.9(43.1) | lb/in(kN/m) | |
| Mooney viscosity ML (1+4) | 125℃ | ASTM D-1646 | 5.9 | Torgue Units |
| tensile strength | @300% Elongation | ASTM D-412 | 493(3.4) | Psi(MPa) |
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | Shore A,15 sec | ASTM D-2240 | 79 | |
| Shore D,15 sec | ASTM D-2240 | 27 | ||
| melt mass-flow rate | ASTM D-1238 | 25 | g/10 min | |
| ASTM D-1238 | 10.0 | g/10 min | ||
| turbidity | ASTM D-1003 | 13@50mils | % | |
| density | ExxonMobil Method | 0.882 | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | 200g | ASTM D-1525 | 159.8(71.0) | ℉(℃) |
| Maximum melt temperature | ExxonMobil Method | 164.7(73.7) | ℉(℃) | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Elongation at Break | @Break | ASTM D-638 | No Break | % |
| Impact strength of cantilever beam gap | 23℃ | ASTM D-256 | No Break | Ft-lb/in(J/m) |
| Bending modulus | 1% secant | ASTM D-790 | 3807(26.2) | Psi(MPa) |
| Impact strength of cantilever beam gap | -40℃ | ASTM D-256 | No Break | Ft-lb/in(J/m) |
| tensile strength | @Break | ASTM D-638 | No Break | Psi(MPa) |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.