POE 8210 EXXONMOBIL USA
EXACT™ 
film
Toughening,High impact resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Other performanceTest ConditionTest MethodEXXONMOBIL USA/8210
Elongation at Break@BreakASTM D-412No Break %
Mooney viscosity ML (1+4)125℃ASTM D-16465.9 Torgue Units
tensile strengthASTM D-624245.9(43.1) lb/in(kN/m)
@100% ElongationASTM D-412407(2.8) Psi(MPa)
@300% ElongationASTM D-412493(3.4) Psi(MPa)
Basic PerformanceTest ConditionTest MethodEXXONMOBIL USA/8210
densityExxonMobil Method0.882
melt mass-flow rateASTM D-123825 g/10 min
Shore hardnessShore D,15 secASTM D-224027
Shore A,15 secASTM D-224079
turbidityASTM D-100313@50mils %
thermal performanceTest ConditionTest MethodEXXONMOBIL USA/8210
Maximum melt temperatureExxonMobil Method164.7(73.7) ℉(℃)
Vicat softening temperature200gASTM D-1525159.8(71.0) ℉(℃)
Physical propertiesTest ConditionTest MethodEXXONMOBIL USA/8210
Bending modulus1% secantASTM D-7903807(26.2) Psi(MPa)
Elongation at Break@BreakASTM D-638No Break %
Impact strength of cantilever beam gap-40℃ASTM D-256No Break Ft-lb/in(J/m)
23℃ASTM D-256No Break Ft-lb/in(J/m)
tensile strength@BreakASTM D-638No Break Psi(MPa)