Material Description
- Material Properties:Talcum powder filling| Talcum powder filling
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
| machinability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shrinkage rate | 3mmt,直径100mm | 1.8 % |
| Basic Performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Water absorption rate | 23°C,60%RH | ASTM D-570 | 0.21 % |
| melt mass-flow rate | ASTM D-1238 | 21 g/10min |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | 23°C | ASTM D-638 | 630 Kgf/cm |
| Elongation at Break | 2mmt | ASTM D-732 | 530 Kgf/cm |
| Rockwell hardness | ASTM D-785 | M84 M Scale | |
| bending strength | 23°C | ASTM D-790 | 1000 Kgf/cm |
| Impact strength of cantilever beam gap | 3.2mmt Stype | ASTM D-1822 | 50 Kgf.cm/cm |
| Bending modulus | 23°C | ASTM D-790 | 3.90 |
| elongation | 23°C | ASTM D-638 | 8 % |
| Impact strength of cantilever beam gap | Notch 3.2mmt | ASTM D-256 | 4 Kgf.cm/cm |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 18.6kgf/cm | ASTM D-648 | 140 °C |
| Combustibility | 0.8mmt | UL 94 | HB |
| Linear coefficient of thermal expansion | 20°C-80°C | ASTM D-696 | 8 |
| Hot deformation temperature | 4.6kgf/cm | ASTM D-648 | 160 °C |
| Melting temperature | 10°C/min | DSC Method | 165 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| filler content | Low % |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Surface resistivity | ASTM D-257 | 1×10 Ω | |
| Volume resistivity | ASTM D-257 | 1×10 Ω.cm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.