Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

POM TC3010 KOLON KOREA
KOCETAL®
--
Talcum powder filling、 Talcum powder filling
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic performance | Test Condition | Test Method | KOLON KOREA/TC3010 |
---|---|---|---|
Water absorption rate | 23°C,60%RH | ASTM D-570 | 0.21 % |
melt mass-flow rate | ASTM D-1238 | 21 g/10min |
Mechanical properties | Test Condition | Test Method | KOLON KOREA/TC3010 |
---|---|---|---|
elongation at break | 2mmt | ASTM D-732 | 530 Kgf/cm |
Impact strength of cantilever beam gap | Notch 3.2mmt | ASTM D-256 | 4 Kgf.cm/cm |
3.2mmt Stype | ASTM D-1822 | 50 Kgf.cm/cm | |
Flexural modulus | 23°C | ASTM D-790 | 3.90 |
Rockwell hardness | ASTM D-785 | M84 M Scale | |
elongation | 23°C | ASTM D-638 | 8 % |
bending strength | 23°C | ASTM D-790 | 1000 Kgf/cm |
tensile strength | 23°C | ASTM D-638 | 630 Kgf/cm |
Electrical performance | Test Condition | Test Method | KOLON KOREA/TC3010 |
---|---|---|---|
Surface Resistivity | ASTM D-257 | 1×10 Ω | |
Volume resistivity | ASTM D-257 | 1×10 Ω.cm |
processability | Test Condition | Test Method | KOLON KOREA/TC3010 |
---|---|---|---|
Shrinkage rate | 3mmt,直径100mm | 1.8 % |
physical property | Test Condition | Test Method | KOLON KOREA/TC3010 |
---|---|---|---|
filler content | Low % |
Thermal performance | Test Condition | Test Method | KOLON KOREA/TC3010 |
---|---|---|---|
Heat distortion temperature | 18.6kgf/cm,HDT | ASTM D-648 | 140 °C |
Linear coefficient of thermal expansion | 20°C-80°C | ASTM D-696 | 8 |
Heat distortion temperature | 4.6kgf/cm,HDT | ASTM D-648 | 160 °C |
combustibility | 0.8mmt | UL 94 | HB |
melting temperature | 10°C/min | DSC Method | 165 °C |