ABS Terluran® HI-12 INEOS STYRO KOREA
287
- Unit Price:US$ 3,454 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:High mobility
- Application Areas:Household goods|Electronic field|Helmet|Electrical appliances|Electrical/Electronic Applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1.02 g/cm³ | |
Melt volume flow rate | ISO 1133 | 14.0 cm3/10min | |
Shrinkage rate | ISO 294-4 | 0.40-0.70 % | |
Water absorption rate | ISO 62 | 1.0 % | |
ISO 62 | 0.21 % |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell hardness | ISO 2039-2 | 101 | |
ball-indentation hardness | ISO 2039-1 | 80.0 Mpa |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL 94 | HB | |
UL 94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
bending strength | ISO 178 | 58.0 Mpa | |
Tensile modulus | ISO 527-2 | 1900 Mpa | |
tensile strength | ISO 527-2 | 40.0 Mpa | |
Tensile strain | ISO 527-2 | 2.7 % |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | 11 kJ/m² | |
ISO 179 | 30 kJ/m² | ||
Impact strength of simply supported beam without notch | ISO 179 | 160 kJ/m² | |
ISO 179 | 无断裂 | ||
Impact strength of cantilever beam gap | ASTM D256 | 35.0 kJ/m² | |
ISO 180/A | 11 kJ/m² | ||
ISO 180/A | 31 kJ/m² |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Compared to the Leakage Tracking Index (CTI) | IEC 60112 | PLC 0 | |
Volume resistivity | IEC 60093 | 1E+15 ohms·cm | |
dielectric constant | IEC 60250 | 2.90 | |
2.80 | |||
Dissipation Factor | IEC 60250 | 5.4E-03 | |
IEC 60250 | 8.2E-03 |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ISO 75-2/B | 102 °C | |
ISO 75-2/A | 97.0 °C | ||
vicat | ISO 306/A50 | 104 °C | |
ISO 306/B50 | 96.0 °C | ||
Linear coefficient of thermal expansion | ISO 11359-2 | 8.0E-5到1.1E-4 cm/cm/°C | |
thermal conductivity | DIN 52612 | 0.17 W/m/K | |
maximum service temperature | 80 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Contact Us
Get App
Top