PA6 Akulon® K223-TP4 DSM HOLAND
290
- Unit Price:US$ 4,499 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:18MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:High impact resistance|High toughness|wear resistant
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
impact performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 18 kJ/m² |
23°C | ISO 179/1eA | 65 kJ/m² | |
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 无断裂 |
23°C | ISO 179/1eU | 无断裂 |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Flammability level | UL 94 | HB | |
Burning wire flammability index | 1.5 mm | IEC 60695-2-12 | 700 °C |
2.0 mm | IEC 60695-2-12 | 700 °C | |
Hot filament ignition temperature | 1.5 mm | IEC 60695-2-13 | 725 °C |
2.0 mm | IEC 60695-2-13 | 725 °C |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ISO 527-2 | 2000 Mpa | |
tensile strength | Yield | ISO 527-2 | 50.0 Mpa |
Tensile strain | Yield | ISO 527-2 | 4.0 % |
Nominal tensile fracture strain | ISO 527-2 | > 50 % | |
Bending modulus | ISO 178 | 1600 Mpa | |
bending strength | ISO 178 | 65.0 Mpa |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 130 °C |
1.8 MPa, Unannealed | ISO 75-2/A | 55.0 °C | |
Linear coefficient of thermal expansion | Flow | ISO 11359-2 | 1.2E-4 cm/cm/°C |
Across Flow | ISO 11359-2 | 1.2E-4 cm/cm/°C |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1.07 g/cm³ | |
Shrinkage rate | 横向Flow | ISO 294-4 | 1.7 % |
Flow | ISO 294-4 | 1.4 % | |
Water absorption rate | Saturation, 23°C | ISO 62 | 8.5 % |
Equilibrium, 23°C, 50% RH | ISO 62 | 2.3 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface resistivity | IEC 60093 | -- ohms | |
Volume resistivity | IEC 60093 | 1.0E+15 ohms·cm | |
Dielectric strength | IEC 60243-1 | 27 KV/mm | |
Relative permittivity | 100 Hz | IEC 60250 | 3.10 |
1 MHz | IEC 60250 | 2.70 | |
Dissipation factor | 100 Hz | IEC 60250 | 3.0E-3 |
1 MHz | IEC 60250 | 0.016 | |
Compared to the anti leakage trace index | IEC 60112 | V |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.