PA6 Durethan®  BKV50 LANXESS GERMANY

354
  • Unit Price:US$ 3,786 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:--
  • Application Areas:--
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

mechanical propertiesTest ConditionTest MethodTest Result
Impact strength of cantilever beam gap23°CISO 180/1A17 kJ/m²
Impact strength of cantilever beam gap-30°CISO 180/1A15 kJ/m²
Impact strength of simply supported beam without notch-30°CISO 179/1eU95 kJ/m²
Impact strength of simply supported beam without notch23°CISO 179/1eU100 kJ/m²
Bending modulus23°CISO 17815000 Mpa
bending strength23°CISO 178340 Mpa
Tensile modulus23°CISO 527-216200 Mpa
Elongation at Break23°CISO 527-22.70 %
tensile strength23°CISO 527-2215 Mpa
Suspended wall beam without notch impact strength-30°CISO 180/1U85 kJ/m²
Suspended wall beam without notch impact strength23°CISO 180/1U85 kJ/m²
thermal performanceTest ConditionTest MethodTest Result
Linear coefficient of thermal expansionTDISO 11359-29E-05 cm/cm/°C
Linear coefficient of thermal expansionMDISO 11359-21.2E-05 cm/cm/°C
Vicat softening temperatureMelting TemperatureISO 11357-3222 °C
Hot deformation temperature1.80MPaAnnealedISO 75-2/Af210 °C
Hot deformation temperature0.45MPaUnannealedISO 75-2/Bf220 °C
Physical propertiesTest ConditionTest MethodTest Result
Shrinkage rateTD2.0mmISO 294-40.60 %
Shrinkage rateMD2.0mmISO 294-40.19 %
Electrical performanceTest ConditionTest MethodTest Result
Dissipation factor相对漏电起痕指数IEC 60112400 V
Dissipation factor23°CIEC 602500.017 1MHz
Dissipation factor23°CIEC 602500.014 100HZ
Dielectric constant23°CIEC 602504.20 1MHz
Dielectric constant23°CIEC 602504.70 100HZ
Dielectric strength1.00mmIEC 60243-135 KV/mm
Volume resistivityIEC 600937E+14 Ω.cm
hardnessTest ConditionTest MethodTest Result
Ball Pressure TestISO 2039-1232 Mpa
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.