plas

PC/ABS CYCOLOY™  C2950HF-111 SABIC INNOVATIVE CHONGQING

244
  • Unit Price:US$ 3,476 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    20MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View

For more details, please contact the supplier!

Material Description

  • Material Properties:Flame retardantHigh mobilityHigh impact resistanceHigh temperature resistanceheat-resisting
  • Application Areas:Electrical fieldElectronic fieldHousehold appliancesHousehold appliancesAutomotive sector
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

impact performanceTest ConditionTest MethodTest Result
Dart impact23°C,EnergyatPeakLoadASTM D376354.2 J
flammabilityTest ConditionTest MethodTest Result
UL flame retardant rating0.76mmUL 94V-2
UL flame retardant rating1.5mmUL 94V-0
UL flame retardant rating2.5mmUL 945VB
UL flame retardant rating3.4mmUL 945VA
Extreme Oxygen IndexASTM D286330 %
mechanical propertiesTest ConditionTest MethodTest Result
bending strengthYield,100mmSpanASTM D79096.5 Mpa
tensile strengthYieldASTM D63864.1 Mpa
elongationYieldASTM D6385.0 %
elongationBreakASTM D63840 %
Bending modulus100mmSpanASTM D7902590 Mpa
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature0.45MPa,Unannealed,6.40mmASTM D648102 °C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTM D64887.8 °C
Hot deformation temperature1.8MPa,Unannealed,6.40mmASTM D64893.3 °C
Vicat softening temperatureASTM D15254113 °C
Linear coefficient of thermal expansionMD:-30to30°CASTM D6967.2E-05 cm/cm/°C
Linear coefficient of thermal expansionTD:-30to30°CASTM D6967.2E-05 cm/cm/°C
thermal conductivityASTMC1770.20 W/m/K
RTI ElecUL 74685.0 °C
RTI ImpUL 74685.0 °C
RTI StrUL 74685.0 °C
Physical propertiesTest ConditionTest MethodTest Result
melt mass-flow rate260°C/2.16kgASTM D123822 g/10min
Shrinkage rateMD:3.20mmInternal Method0.40-0.60 %
Shrinkage rateTD:3.20mmInternal Method0.40-0.60 %
Water absorption rate24hrASTM D5700.10 %
Water absorption rateEquilibrium,23°CASTM D5700.40 %
Electrical performanceTest ConditionTest MethodTest Result
Dissipation factor50HzASTM D1505.2E-03
Dissipation factor60HzASTM D1505.2E-03
Dissipation factor1MHzASTM D1507.1E-03
Arc resistanceASTM D495PLC6
Compared to the anti leakage trace indexCTIUL 746PLC 2
High arc combustion indexHAIUL 746PLC 0
High voltage arc tracing rateHVTRUL 746PLC 3
Hot wire ignitionHWIUL 746PLC 2
Surface resistivityASTM D257>1.0E+16 ohms
Volume resistivityASTM D2571.6E+17 ohms·cm
Dielectric strength3.20mm,inOilASTM D14924 KV/mm
Dielectric constant50HzASTM D1502.80
Dielectric constant60HzASTM D1502.80
Dielectric constant1MHzASTM D1502.70
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessR-ScaleASTM D785121
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.