PPO NORYL™ EN185-701 SABIC INNOVATIVE US
172
- Unit Price:US$ 3,768 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:Conductive|Glass fiber reinforced
- Application Areas:electromagnetic shielding
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D792 | 1.08 g/cm³ | |
Water absorption rate | ASTM D570 | 0.070 % |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell hardness | ASTM D785 | 113 |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL 94 | V-1 | |
UL 94 | V-0 | ||
Radiation board grade | UL Unspecified | TRUE |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTM D638 | 42.0 Mpa | |
elongation | ASTM D638 | 50 % | |
Flexural modulus | ASTM D790 | 2270 Mpa | |
bending strength | ASTM D790 | 67.0 Mpa |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of cantilever beam gap | ASTM D256 | 160 J/m | |
ASTM D256 | 390 J/m | ||
Dart impact | ASTM D3029 | 13.0 J | |
ASTM D3029 | 24.0 J |
squeeze out | Test Condition | Test Method | Test Result |
---|---|---|---|
drying temperature | 90 to 100 °C | ||
drying time | 2.0 to 4.0 hr | ||
Suggested maximum moisture content | 0.020 % | ||
Temperature in Zone 1 of the material cylinder | 170 °C | ||
Temperature in Zone 2 of the material cylinder | 170 °C | ||
Temperature in Zone 3 of the material cylinder | 190 °C | ||
Temperature in Zone 4 of the material cylinder | 190 °C | ||
Joint temperature | 205 °C | ||
Melt Temperature | 195 to 210 °C | ||
die temperature | 205 °C |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
dielectric strength | ASTM D149 | 25 KV/mm | |
dielectric constant | ASTM D150 | 2.80 | |
ASTM D150 | 2.80 | ||
Dissipation Factor | ASTM D150 | 4.0E-3 | |
ASTM D150 | 4.0E-3 | ||
IEC 60250 | 3.5E-3 | ||
arc resistance | ASTM D495 | PLC 7 | |
Compared to the Leakage Tracking Index (CTI) | UL 746 | PLC 2 | |
High arc combustion index (HAI) | UL 746 | PLC 0 | |
High Voltage Arc Traceability Rate (HVTR) | UL 746 | PLC 4 | |
Hot wire ignition (HWI) | UL 746 | PLC 1 |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ASTM D648 | 93.0 °C | |
ASTM D648 | 82.0 °C | ||
Linear coefficient of thermal expansion | ASTM E831 | 7.4E-5 cm/cm/°C | |
RTI Elec | UL 746 | 50.0 °C | |
RTI Imp | UL 746 | 50.0 °C | |
RTI | UL 746 | 50.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.