PBT VALOX™  357U-1001 SABIC INNOVATIVE SHANGHAI

329
  • Unit Price:US$ 4,779 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    231.8MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View

For more details, please contact the supplier!

Material Description

  • Material Properties:Flame retardantUV resistanceImpact modification
  • Application Areas:Electrical fieldElectronic fieldElectrical appliancesmedicineMedical suppliesNursing suppliesPlastic bagLiquid handlingLawn equipmentGarden equipmentNon specific foodOutdoor applicationsIndustrial applicationsHousehold goodsArchitectural application fieldLighting applications
  • Color:--
  • Grade:Injection grade

Material Certification

UL

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest Result
Specific volumeASTM D7920.750 cm³/g
Shrinkage rate内部方法0.80 - 1.1 %
Shrinkage rate内部方法1.0 - 1.4 %
Shrinkage rate内部方法0.90 - 1.3 %
Shrinkage rate内部方法1.2 - 1.6 %
Water absorption rateASTM D5700.080 %
Outdoor applicabilityUL 746Cf1
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessASTM D785117
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94HB
UL flame retardant ratingUL 94V-0
UL flame retardant ratingUL 945VA
Limiting Oxygen IndexASTM D286330 %
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength ASTM D63848.0 Mpa
tensile strength ASTM D63848.0 Mpa
elongationASTM D638110 %
Flexural modulusASTM D7902060 Mpa
bending strengthASTM D79082.0 Mpa
bending strengthASTM D79082.0 Mpa
Impact resistanceTest ConditionTest MethodTest Result
Suspended wall beam without notch impact strengthASTM D48123200 J/m
Dart impactASTM D302943.0 43.0 J
Electrical performanceTest ConditionTest MethodTest Result
Volume resistivityASTM D257> 1.2E+16 ohms·cm
dielectric strengthASTM D14925 KV/mm
dielectric strengthASTM D14919 KV/mm
dielectric strengthASTM D14919 KV/mm
dielectric constantASTM D1503.20
dielectric constantASTM D1503.20
Dissipation FactorASTM D1503.0E-3
Dissipation FactorASTM D1500.030
arc resistanceASTM D495PLC 6
Compared to the Leakage Tracking Index (CTI)UL 746PLC 2
High arc combustion index (HAI)UL 746PLC 3
High Voltage Arc Traceability Rate (HVTR)UL 746PLC 3
Hot wire ignition (HWI)UL 746PLC 2
injectionTest ConditionTest MethodTest Result
drying temperature120 °C
drying time3.0 to 4.0 hr
Suggested maximum moisture content0.020 %
Suggested injection volume40 to 80 %
Temperature at the rear of the barrel240 to 255 °C
Temperature in the middle of the barrel245 to 260 °C
Temperature at the front of the material cylinder250 to 265 °C
Spray nozzle temperature245 to 260 °C
Processing (melt) temperature250 to 265 °C
Temperature50 to 75 °C
Back pressure0.300 to 0.700 Mpa
screw speed50 to 100 rpm
Exhaust hole depth0.025 to 0.038 mm
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D648137 °C
Heat distortion temperatureASTM D64898.0 °C
Linear coefficient of thermal expansionASTM E8319.2E-5 cm/cm/°C
Linear coefficient of thermal expansionASTM E8311.2E-4 cm/cm/°C
RTI ElecUL 746120 °C
RTI ImpUL 746120 °C
RTIUL 746140 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.