Material Description
- Material Properties:High surface finish|filler|Mineral filler|20%|Filler by weight
- Application Areas:Car bumper|Automotive External Parts|Car exterior decoration|Automotive sector|Automotive External Parts
- Color:--
- Grade:Injection grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | NoBreak | |
| Charpy Notched Impact Strength | -20°C | ISO 179/1eA | 4.0 | kJ/m² |
| 23°C | ISO 179/1eA | 30 | kJ/m² | |
| -30°C | ISO 179/1eA | 3.0 | kJ/m² | |
| Impact strength of cantilever beam gap | -20°C | ISO 180/1A | 4.0 | kJ/m² |
| 23°C | ISO 180/1A | 34 | kJ/m² | |
| Impact strength of simply supported beam without notch | -20°C | ISO 179/1eU | 96 | kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile strain | Yield | ISO 527-2/50 | 4.5 | % |
| Break | ISO 527-2/50 | 100 | % | |
| tensile strength | Yield | ISO 527-2/50 | 19.5 | Mpa |
| bending strength | ISO 178 | 28.0 | Mpa | |
| Bending modulus | ISO 178 | 1900 | Mpa | |
| Tensile modulus | ISO 527-2/1 | 1800 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 105 | °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 56.0 | °C | |
| Vicat softening temperature | -- | ISO 306/B50 | 49.0 | °C |
| -- | ISO 306/A50 | 140 | °C | |
| Linear coefficient of thermal expansion | MD:-30to80°C | Internal Method | 5.2E-05 | cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | --2 | Internal Method | 0.80 | % |
| 90°C,2hr | Internal Method | 0.10 | % | |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 10 | g/10min |
| density | ISO 1183 | 1.05 | g/cm³ | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Ball Pressure Test | H132/10 | ISO 2039-1 | 43.0 | Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.