PA66 Zytel® 105F BK010 DUPONT USA
309
- Unit Price:US$ 4,480 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:74.1MT
- Delivery Terms:FOB
- Port of Loading :Guangzhou port, China
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:Photostability|Short molding cycle|Good weather resistance
- Application Areas:Electronic and electrical accessories|Automotive components
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
| other | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| characteristic | PA66.耐候.含细微分散碳黑 | |||
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 55 | kJ/m² |
| 23°C | ISO 179/1eU | 45 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 0.71mm | UL 94 | V-2 | |
| 1.5mm | UL 94 | V-2 | ||
| Fogging-G-value | condensate | ISO 6452 | 0.0 | g |
| FMVSS flammability | FMVSS302 | SE | ||
| Extreme Oxygen Index | ISO 4589-2 | 27 | % | |
| UL flame retardant rating | 1.5mm | IEC 60695-11-10,-20 | V-2 | |
| 0.71mm | IEC 60695-11-10,-20 | V-2 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile creep modulus | 1000hr | ISO 899-1 | -- | Mpa |
| 1hr | ISO 899-1 | -- | Mpa | |
| Nominal tensile fracture strain | ISO 527-2 | 24 | % | |
| Tensile strain | Yield | ISO 527-2 | 4.3 | % |
| tensile strength | Yield | ISO 527-2 | 85.0 | Mpa |
| Tensile modulus | ISO 527-2 | 3200 | Mpa | |
| Charpy Notched Impact Strength | ASTM D256/ISO 179 | 5 | kg·cm/cm(J/M)ft·lb/in | |
| ASTM D256/ISO 179 | NB | kg·cm/cm(J/M)ft·lb/in | ||
| ASTM D256/ISO 179 | 70 | kg·cm/cm(J/M)ft·lb/in | ||
| ASTM D256/ISO 179 | 4 | kg·cm/cm(J/M)ft·lb/in | ||
| Elongation at Break | ASTM D638/ISO 527 | 20 | % | |
| Tensile modulus | ASTM D638/ISO 527 | 3200 | kg/cm²(MPa)[Lb/in²] | |
| tensile strength | ASTM D638/ISO 527 | 85 | kg/cm²(MPa)[Lb/in²] | |
| Bending modulus | ASTM D790/ISO 178 | 2900 | kg·cm/cm(J/M)ft·lb/in | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 1.1E-04 | cm/cm/°C |
| MD | ISO 11359-2 | 1E-04 | cm/cm/°C | |
| Melting temperature | ISO 11357-3 | 263 | °C | |
| Vicat softening temperature | ISO 306/B50 | 240 | °C | |
| Glass transition temperature | ISO 11357-2 | 60.0 | °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 70.0 | °C |
| 0.45MPa,Unannealed | ISO 75-2/B | 205 | °C | |
| Combustibility (rate) | UL 94 | V-2 | ||
| Hot deformation temperature | HDT | ASTM D648/ISO 75 | 205 | ℃(℉) |
| HDT | ASTM D648/ISO 75 | 70 | ℃(℉) | |
| Melting temperature | 263 | ℃(℉) | ||
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Top out temperature | 190 | °C | ||
| Stickiness | ISO 307 | 145 | cm³/g | |
| Water absorption rate | Equilibrium,23°C,2.00mm,50%RH | ISO 62 | 2.7 | % |
| Saturation,23°C,2.00mm | ISO 62 | 8.5 | % | |
| Shrinkage rate | MD | ISO 294-4 | 1.3 | % |
| TD | ISO 294-4 | 1.3 | % | |
| density | ASTM D792/ISO 1183 | 1.14 | ||
| Shrinkage rate | ASTM D955 | 1.5(流动.3.2mm) | % | |
| Water absorption rate | ASTM D570/ISO 62 | 2.7 | % | |
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| Odor | VDA270 | 2.50 | ||
| EmissionofOrganicCompounds | VDA277 | 6.60 | µgC/g |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.