PA66 TECHNYL® A 60G1 V30 SOLVAY FRANCE
6
- Unit Price:US$ 5,350 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:100MT
- Delivery Terms:FOB
- Port of Loading :Shenzhen Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Transaction Guarantee:
Supplier Information
Guangdong Beiyan Chemical New Material Co., Ltd.
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 9.5 | kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 85 | J/m |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 60 | kJ/m² |
| -30°C | ISO 179/1eU | 60 | kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 10 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 0.8 mm | UL 94 | V-0 | |
| 1.6 mm | UL 94 | V-0 | ||
| 3.2 mm | UL 94 | V-0 | ||
| Burning wire flammability index | 0.8 mm | IEC 60695-2-12 | 960 | °C |
| 1.6 mm | IEC 60695-2-12 | 960 | °C | |
| 3.2 mm | IEC 60695-2-12 | 960 | °C | |
| Hot filament ignition temperature | 0.8 mm | IEC 60695-2-13 | 775 | °C |
| Extreme Oxygen Index | ISO 4589-2 | 33 | % | |
| European Railways Certifications | R22 | EN 45545-2 | HL3 | |
| R23 | EN 45545-2 | HL3 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | 23°C | ISO 178 | 255 | Mpa |
| 23°C | ASTM D790 | 225 | Mpa | |
| Bending modulus | 23°C | ASTM D790 | 10000 | Mpa |
| elongation | Break, 23°C | ISO 527-2 | 2.3 | % |
| Break, 23°C | ASTM D638 | 3.0 | % | |
| tensile strength | Break, 23°C | ISO 527-2/1A | 150 | Mpa |
| Break, 23°C | ASTM D638 | 140 | Mpa | |
| Tensile modulus | 23°C | ISO 527-2/1A | 10200 | Mpa |
| injection | Test Condition | Test Method | Test Result | Test Unit |
| Temperature at the front of the material cylinder | 270 to 280 | °C | ||
| Mold temperature | 60 to 90 | °C | ||
| drying temperature | 80 | °C | ||
| Suggested maximum moisture content | 0.20 | % | ||
| Temperature at the rear of the barrel | 265 to 275 | °C | ||
| Temperature in the middle of the barrel | 265 to 275 | °C | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Melting temperature | ISO 11357-3 | 263 | °C | |
| Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/Af | 245 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Thermogravimetric analysis (TGA) | 1%失重温度 | NF F16-101 | I3 | |
| Outdoor applicability | 全部 | UL 746C | f1 | |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 1.8 | % |
| Saturation, 23°C | ISO 62 | 4.3 | % | |
| 24 hr, 23°C | ISO 62 | 0.73 | % | |
| Shrinkage rate | Flow | ISO 294-4 | 0.35 | % |
| 横向Flow | ISO 294-4 | 1.0 | % | |
| density | ISO 1183/A | 1.46 | g/cm³ | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric strength | 0.800 mm | IEC 60243-1 | 38 | KV/mm |
| Volume resistivity | IEC 60093 | 6.0E+14 | ohms·cm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Other Prices
| Supplier | Unit Price |
|---|---|
| ASIAPLAS | US$ 5140 /MT |